Please wait a minute...
Acta Metall Sin  2007, Vol. 43 Issue (8): 807-812     DOI:
Research Articles Current Issue | Archive | Adv Search |
Effect of deep-cooling and measurement temperature on damping capacity of Fe-Mn alloy
Shu-Ke Huang;LI Ning;;;
四川大学制造科学与工程学院
Cite this article: 

Shu-Ke Huang; LI Ning. Effect of deep-cooling and measurement temperature on damping capacity of Fe-Mn alloy. Acta Metall Sin, 2007, 43(8): 807-812 .

Download:  PDF(629KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  In order to disclosure the high damping mechanism of Fe-Mn alloy, the effect of deep-cooling and measurement temperature on damping capacity was studied, by measuring stacking fault probability and using G-L dislocation model. The damping capacity was measured using reversal torsion pendulum. The stacking fault probability and volume fraction of ε-martensite were determined using XRD. The microstructure was observed using SEM. The results indicated that the high damping mechanism was determined by the movement of Shockley partial dislocation, and not by ε-martensite. Because Deep-cooling increased the stacking fault probability in γ-austenite and ε-martensite, the number of Shockley partial dislocations also increased and the damping capacity of Fe-Mn alloy was improved. Higher temperature could decrease the unpinning stress between Shockley partial dislocation and weak pinning points. At a certain strain amplitude, therefore, with the temperature increased, the number of unpinning Shockley partial dislocations was more and the damping capacity of Fe-Mn alloy was improved.
Key words:  damping alloy      Fe-Mn      Shockley partial dislocation      stacking fault probability      deep-cooling      
Received:  04 December 2006     
ZTFLH:  TG135.7  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2007/V43/I8/807

[1]Pulino-Sagradi D,Sagradi M, Karimi A,Martin J L.Scr Mater,1998;39:131
[2]Wu S K,Lin H C.J Alloy Compd,2003;355:72
[3]Liu Y C,Yang G C,Lu L L,Yang L S.J Mater Process ??Technol,1999;87:53
[4]G(?)ken J,Riehemann W.Mater Sci Eng,2004;A370:417
[5]Balk S H.Nucl Eng Des,2000;198:241
[6]De A K,Cabanas N,de Cooman B C.Z Metallkd,2002; 93:228
[7]Wu X C,Zhang J H,Xu Z Y.J Shanghai Jiaotong Univ, 1998;32(2):1 (吴晓春,张骥华,徐祖耀.上海交通大学学报,1998;32(2):1)
[8]Jun J H,Choi C S.Mater Sci Eng,1998;A252:133
[9]Huang S K,Li N,Wen Y H,Ding S,Teng J.J Sichuan Univ(Eng Sci Ed),2007;39:123 (黄姝珂,李宁,文玉华,丁胜,滕劲.四川大学学报(工程科学版),2007;39:123)
[10]Lee Y K,Jun J H,Choi C S.ISIJ Int,1997;37:1023
[11]GB/T 13665-1992.Test Method for Damping Capacity of Metallic Damping Materials-Torsion Pendulum Method and Flexural Resonance Method.Beijing:Standards Press of China,1992 (GB/T 13665-1992.金属阻尼材料阻尼本领试验方法—扭摆法和弯曲共振法.北京:中国标准出版社,1992)
[12]Lee Y K,Baik S H,Kim J C,Choi C S.J Alloy Compd, 2003;355:10
[13]Warren B E.X-ray Diffraction.Reading,Mass:Addison- Wesley,1969:275
[14]Ramous E.Z Metallkd,1974;65:515
[15]He G,Zhao H B,Rong Y H,Guo Z H,Chen S P,Xu Z Y.J Shanghai Jiaotong Univ,1999;33:765 (何刚,赵恒北,戎咏华.郭正洪,陈世朴,徐祖耀.上海交通大学学报,1999;33:765)
[16]Granato A,L(?)cke K.J Appl Phys,1956;27:583
[17]Teutonico L J,Granato A V,L(?)cke K.J Appl Phys,1964; 35:220
[18]Lee Y K,Jun J H,Choi C S.Ser Mater,1996;35:825
[19]Wen Y H,Li N,Tu M J.J Mater Sci Technol,2000;16: 424
[20]Lücke K Granato A V,Teutonico L J.J Appl Phys,1968; 39:5181
[1] DING Hua, ZHANG Yu, CAI Minghui, TANG Zhengyou. Research Progress and Prospects of Austenite-Based Fe-Mn-Al-C Lightweight Steels[J]. 金属学报, 2023, 59(8): 1027-1041.
[2] REN Ping, CHEN Xingpin, WANG Cunyu, YU Feng, CAO Wenquan. Effects of Pre-Strain and Two-Step Aging on Microstructure and Mechanical Properties of Fe-30Mn-11Al-1.2C Austenitic Low-Density Steel[J]. 金属学报, 2022, 58(6): 771-780.
[3] WANG Shihong, LI Jian, CHAI Feng, LUO Xiaobing, YANG Caifu, SU Hang. Influence of Solution Temperature on γ→ε Transformation and Damping Capacity of Fe-19Mn Alloy[J]. 金属学报, 2020, 56(9): 1217-1226.
[4] Xingpin CHEN,Wenjia LI,Ping REN,Wenquan CAO,Qing LIU. Effects of C Content on Microstructure and Properties ofFe-Mn-Al-C Low-Density Steels[J]. 金属学报, 2019, 55(8): 951-957.
[5] YANG Fuqiang, SONG Renbo, SUN Ting, ZHANG Leifeng, ZHAO Chao, LIAO Baoxin. MICROSTRUCTURE AND MECHANICAL PROPER- TIES OF Fe-Mn-Al LIGHT-WEIGHT HIGH STRENGTH STEEL[J]. 金属学报, 2014, 50(8): 897-904.
[6] ZHU Xuemei CAO Xuemei LIU Ming LEI Mingkai ZHANG Yansheng. AN ANTIFERROMAGNETIC Fe24Mn4Al5Cr COVAR ALLOY IMPULSE--PASSIVATED BY AN ALTERNATING CURRENT VOLTAGE OVERLAPPING A DIRECT CURRENT VOLTAGE AND ITS CORROSION RESISTANCE[J]. 金属学报, 2012, 48(11): 1357-1364.
[7] PENG Huabei LIU Gang WEN Yuhua SUN Panpan LI Ning. A TRAINING-FREE CAST Fe-Mn-Si-Cr-Ni SHAPE MEMORY ALLOY BASED ON FORMATION OF MARTENSITE IN A DOMAIN MANNER I. Idea and realization[J]. 金属学报, 2010, 46(3): 282-287.
[8] LIU Gang PENG Huabei WEN Yuhua YANG Kun LI Ning. A TRAINING-FREE CAST Fe-Mn-Si-Cr-Ni SHAPE MEMORY ALLOY BASED ON FORMATION OF MARTENSITE IN A DOMAIN MANNER II. Influence of annealing on shape memory effect[J]. 金属学报, 2010, 46(3): 288-293.
[9] HUANG Shuke LIU Jianhui LI Chang'an ZHOU Danchen LI Ning WEN Yuhua. EFFECT OF PRE-DEFORMATION ON STACKING FAULT PROBABILITY AND DAMPING CAPACITY OF Fe-Mn ALLOY[J]. 金属学报, 2009, 45(8): 937-942.
[10] Xu Yun-Wei; MA Tian-Yu; Mi YAN. MAGNETOSTRICTION IN ANTIFERROMAGNETIC Fe1-xMnx (0.30 ≤ x ≤ 0.55) ALLOYS[J]. 金属学报, 2008, 44(10): 1235-1237 .
[11] . [J]. 金属学报, 2007, 43(6): 648-652 .
[12] LIU Xiangjun; LIN Xinyuan; CHEN Shiren (Institute for Materials Research; Fuzhou University; Fuzhou 350002)Correspondent: CHEN Shiren; professor Tel: (0591)3728486; Fax. (0591)3713866;E-mail: material@fzu. edu.cn. STICKING FAULT ENERGY CALCULATING OF TWO KINDS OF STAINLESS IRON BASED SHAPE MEMORY ALLOYS[J]. 金属学报, 1998, 34(9): 903-907.
[13] RONG Lijian; LI Yiyi;SHI Changxu (Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015). EFFECT OF PRE-STRAINING TEMPERATURE OF AUSTENITE ON IMPROVEMENT OF SME IN Fe-Mn-Si ALLOY[J]. 金属学报, 1995, 31(3): 125-129.
[14] GUO Shangxing; DONG Yuanchi(East China Institute of Metallurgy; Ma'anshan 243002). THERMODYNAMICS OF Fe-Mn-C-P MELTS CONTAINING HIGH Mn[J]. 金属学报, 1995, 31(18): 241-246.
[15] LIU Xingjun; HAO Shiming; SUN Rongyao; (Northeast University of Technology; Shenyang). ISOTHERMAL SECTION AT 1000 AND 1100℃ OF Fe-Mn-AI SYSTEM PHASE DIAGRAM[J]. 金属学报, 1992, 28(7): 50-54.
No Suggested Reading articles found!