| (Fe-B-Y)-based quinary bulk metallic glasses designed using cluster line criterion |
| CHEN Wei-Rong;;;Qingyu Zhang; |
| 大连理工大学;大连大学 |
|
Cite this article:
CHEN Wei-Rong; Qingyu Zhang. (Fe-B-Y)-based quinary bulk metallic glasses designed using cluster line criterion. Acta Metall Sin, 2007, 43(8): 797-802 .
|
|
|
Abstract This work investigates the glass formation of Fe-B-Y-based multicomponent alloys designed using a cluster line approach. Cluster lines Fe8B3-Y, Fe8B2-Y, Fe83B17-Y, Fe6B-Y and Fe9B-Y intersect with cluster line Fe12Y-B at five compositions in the Fe-B-Y phase diagram that are taken as basic compositions. Further minor alloying by additions of 2 at.% Nb and 2 at.% M (M=Ti, Hf, Ta, Mo, Ni, and Sn) was designed and alloy rods were synthesized with a diameter of 3mm by suction-casting in copper mold. A. Considering mass loss of B and Y during arc melting, the ingots were all weighted after each melting and the final compositions were revised accordingly. When M=Ti, Hf, Ta and Mo, the quinary alloys form BMGs at compositions close to the Fe8B3-Y cluster line. This signifies that the close-packed Archimedes octahedral antiprism Fe8B3 is the basic atomic cluster that favors glass formation. The best glass-forming composition is (Fe69.9B24.6Y5.5)96Nb2Ti2 with Tg=944K, Tx=997K, Trg=0.666. When M=Ni and Sn, no glass formation was observed.
|
|
Received: 08 December 2006
|
|
|
[1]Inoue A,Shen B L,Takeuchi A.Mater Trans,2006;47: 1275 [2]Shen B L,Akiba M,Inoue A.Appl Phys Lett,2006;88: 131907 [3]Inoue A,Shinohara Y,Gook J S.Mater Trans JIM,1995; 36:1427 [4]Inoue A,Zhang T,Takeuchi A.Appl Phys Lett,1997;71: 464 [5]Inoue A,Chen B.Mater Trans,2002;43:766 [6]Inoue A,Nishiyama N,Matsuda T.Mater Trans JIM, 1996;37:181 [7]Inoue A,Zhang T,Mosumoto T.Mater Trans JIM,1990; 31:177 [8]Inoue A,Zhang W.Mater Trans,2002;43:2921 [9]Lin C Y,Tien H Y,Chin T S.Appl Phys Lett,2005;86: 162501 [10]Wang Y M,Zhang X F,Qiang J B,Wang Q,Wang D H, Li D J,Shek C H,Dong C.Scr Mater,2004;50:829 [11]Zhang X F,Wang Y M,Qiang J B,Wang Q,Wang D H, Li D J,Shek C H,Dong C.Intermetallics,2004;12:1275 [12]Wang Q,Wang Y M,Qiang J B,Zhang X F,Shek C H, Dong C.Intermetallics,2004;12:1229 [13]Wang Q,Qiang J B,Wang Y M,Xia J H,Lin Z,Zhang X F,Dong C. Acta Phys Sin,2006;55:378 (王清,羌建兵,王英敏,夏俊海,林哲,张新房,董闯.物理学报,2006;55:378) [14]Wu J,Wang Q,Qiang J B,Chen F,Dong C,Wang Y M, Shek C H.J Mater Res,2007:22:573 [15]Dong C,Qiang J B,Wang Y M,Jiang N,Wu J,Thiel P. Philos Mag,2006;86:263 [16]Inoue A,Takeuchi A,shen B.Mater Trans.2001;42:970 [17]Xia J H,Qiang J B,Wang Y M,Wang Q,Dong C.Appl Phys Lett,2006;88:101907 [18]Inoue A.Mater Trans JIM,1995;36:866 [19]Inoue A.Mater Sci Eng,2001;A304-306:1 [20]Miracle D B,Senkov O N,Sanders W S,Kending K L. Mater Sci Eng,2004:A375-377:150 [21]Miracle D B.J Non-Cryst Solids,2004;342:89 [22]Miracle D B,Sanders W S.Philos Mag,2003;83:2409 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |