| Evolutions of Structure, Texture And Mechanical Property of IF Steel Subjected to Surface Mechanical Attrition Treatment |
| LI Sijun; LIU Gang;ZHOU Lei; WANG Fu; ZUO Liang |
| School of Materials and Metallurgy; Northeastern University |
|
Cite this article:
LI Sijun; LIU Gang; ZHOU Lei; WANG Fu; ZUO Liang. Evolutions of Structure, Texture And Mechanical Property of IF Steel Subjected to Surface Mechanical Attrition Treatment. Acta Metall Sin, 2007, 43(7): 744-748 .
|
|
|
|
|
Received: 23 October 2006
|
|
|
[1]Lu K,L(?)J.J Matt Sci Technol,1999;15:193 [2]Lu K,L(?)J.Mater Sci Eng,2004;A375-377:38 [3]Liu G,L(?)J,Lu K.Scr Mater,2001;44:1791 [4]Yong X P,Liu G,Lu K,L(?)J.J Mater Sci Technol,2003; 19:1 [5]Zhang H W,Liu G,Hei Z K,L(?)J,Lu,K.Acta Metall Sin,2003;39:342 (张洪旺,刘刚,黑祖昆,吕坚,卢柯.金属学报,2003; 39:342) [6]Wu X,Tao N,Hong Y,Xu B,L(?)J,Lu K.Acta Mater, 2002;50:2075 [7]Zhu K Y,Vassel A,Brisset F,Lu K,L(?)J.Acta Mater, 2004;52:4101 [8]Wu X,Tao N,Hong Y,Liu G,Xu B,L(?)J,Lu K.Acta Mater,2005;53:681 [9]Wang K,Tao N R,Liu G,L(?)J,Lu K.Acta Mater,2006; 54:5281 [10]Tao N R,Wang Z B,Tong W P,Sui M L,L(?)J,Lu K. Aeta Mater,2002;50:4603 [11]Zhang H W,Hei Z K,Liu G,L(?)J,Lu K.Acta Mater, 2003;51:1871 [12]L(?)A Q,Liu G,Liu C M.Acta Metall Sin,2004;40:943 (吕爱强,刘刚,刘春明.金属学报.2004;40;943) [13]Tsuji N,Ueji R,Minamino Y.Scr Mater,2002;47:69 [14]Kamikawa N,Tsuji N,Minamino Y.Sci Technol Adv Mater,2004;5:163 [15]Han B Q,Yue S.J Mater Process Technol,2003;136:100 [16]Sato M,Tsuji N,Minamino Y.Sci Technol Adv Mater, 2004;5:145 [17]Liang Z D,Xu J Z,Wang F.Proc ICOTOM 6,Tokyo, Japan,1981:1259 [18]Yang D,Wang X,Mao W M,Zhang S H.J Univ Sci Technol Beijing,1994;16:250 (杨弟,王绪,毛为民,章守华.北京科技大学学报,1994; 16:250) [19]Wang A X,Liu G,Zhou L,Wang K,Yang X H,Li Y. Acta Metall Sin,2005;41:577 (王爱香,刘刚,周蕾,王科,杨晓华,李瑛.金属学报,2005;41:577)B |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|