Abstract In this paper the grain orientation of as-cast AZ80 magnesium alloy during multiple forging process was studied. The results show that preferred orientation during plastic flow mostly result from grain rotation and orientation shift. In the case of very small deformation without any initiation of new grains, slipping and twinning resulting in grain rotation may lead to the formation of relatively strong basal preferred orientation. Basal preferred orientation changes with the applied loading axis rotation and is aligned parallel to the compression direction during the first 9 passes except the 4th one. After 10 passes of multiple forging processing, the final orientation distribution is close to random. Forging temperature and deformation mode have an important influence on the evolution of grain orientation while pass strain does not. Both decreasing deformation temperature in some degree and multi-directional deformation mode can promote the formation of strong basal orientation.
|
|
Received: 23 October 2006
|
|
|
[1]Chen Z H.Wrought Magnesium Alloy.Beijing:Chemical Industry Press,2005 (陈振华.变形镁合金.北京:化学工业出版社,2005) [2]Chen Z H,Xia W J,Cheng Y Q,Fu D F.Chin J Nonfer- rous Met,2005;15:1 (陈振华,夏伟军,程永奇,傅定发.中国有色金属学报,2005; 15:1) [3]Robert G,Matthias M F,Güter G.Mater Sci Eng,2005; A395:338 [4]Watanabe H,Mukai T,Ishikawa K.J Mater Sci,2004;39: 1477 [5]Cheng Y Q,Chen Z H,Xia W J,Fu D F.Chin J Nonfer- ??rous Met,2005;15:1369 (程永奇,陈振华,夏伟军,傅定发.中国有色金属学报,2005; 15:1369) [6]Mironov S Y,Salishchev G A,Myshlyaev M M,Pippan R.Mater Sci Eng,2006;A418:257 [7]Ringeval S,Piot D,Desrayaud C,Driver J H.Acta Mater, 2006;54:3095 [8]Guo Q,Yan H G,Chen Z H,Zhang H.Acta Metall Sin, 2006;42:739 (郭强,严红革,陈振华,张辉.金属学报,2006;42:739) [9]Carlos N,Tomé,George C K.Mater Sci Forum,2005; 495-497:1001 [10]Mark D N,Matthew R B.Scr Mater,2004;51:881 [11]del Valle J A,Perez-Prado M T,Ruano O A.Metall Mater Trans,2005;36A:1427 [12]Bohlen J,Li S B,Swiosteck J,Letzig D,Brokmeier H G, Kainer K U.Scr Mater,2005;53:259 [13]Yang X Y,Miura H,Sakai T.Mater Trans,2003;44:197 [14]Galiyev A,Kaibyshev R,Gottstein G.Acta Mater,2001; 49:1199 [15]del Valle J A,Perez-Prado M T,Ruano O A.Mater Sci Eng,2003;A355:68 [16]Perez-Prado M T,del Valle J A,Contreras J M,Ruano O A.Scr Mater,2004;50:661 [17]Perez-Prado M T,del Valle J A,Ruano O A.Scr Mater, 2004;50:667 [18]Tanno Y,Mukai T,Asakawa M.Mater Sci Forum,2003; 419-422:359 [19]Wu S K,Chou T S,Wang J Y.Mater Sci Forum,2003; 419-422:527 [20]Sitdikov O,Sakai T,Goloborodko A,Miura H,Kaibyshev R.Mater Trans,2004;45:2232 [21]Sitdikov O,Sakai T,Goloboradko A,Miura H.Scr Mater, 2004;51:175 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|