Abstract Molten magnesium has been oxidized in the atmospheres of air containing HFC-134a in the temperature range of 660℃~800℃. The oxidation kinetic curves of molten magnesium have been measured by the weight gain method. The oxidation products have been characterized by XRD and EDS. The results show that the oxidation kinetics of molten magnesium are greatly influenced by the concentration of HFC-134a and temperature. The curve of oxidation weight gain against time is linear and the oxidation film consists mainly of MgO when the concentration of HFC-134a in air is low. The oxidation follows parabolic rate law and the film consists mainly of MgF2 when the concentration of HFC-134a in air is high. An oxidation mechanism of molten magnesium in air containing HFC-134a has been proposed to account for the experimental results.
[1]Erickson S C,King J F,Mellerud T.Found Manage Tech- nol,1998;126:38 [2]Ricketts N J,Cashion S P.Magnesium Technology 2001. ??Warrendale,PA:TMS,2001:31 [3]Ricketts N J,Cashion S P,Bailey R.Proc 1st Int Light Met Technol Conf,Brisbane,Australia:CAST,2003:275 [4]Lyon P,Rogers P D,King J F,Cashion S P,Ricketts N J.In:Kaplan H ed.,Magnesium Technology 2003,War- rendale,PA:TMS,2003:11 [5]Won H,Jae E L,Young J K.Mater Sci Forum,2005; 475-479:2543 [6]Pettersen G,Ovrelid E,Tranell G,Fenstad J,Gjestland H.Mater Sci Eng,2002;A332:285 [7]Liu X L,Xiong S M.Rare Met Mater Eng,2006;35:1396 (刘晓龙,熊守美.稀有金属材料与工程,2006;35:1396) [8]Huang Z Q,Zeng Y W,Mao M X.Spec Cast Nonferrous Alloys,2006;26:532 (黄志强,曾一文,毛明现.特种铸造及有色合金,2006;26: 532) [9]Salas O,Vlach K C,Levi C G,Jayaram V.J Mater Res, 1991;6:1964 [10]Zeng X,Wang Q,Lu Y,Ding W,Zhu Y,Zhai C,Lu C, Xu X.Mater Sci Eng,2001;A301:154