Please wait a minute...
Acta Metall Sin  2007, Vol. 43 Issue (11): 1207-1210     DOI:
Research Articles Current Issue | Archive | Adv Search |
Cite this article: 

. . Acta Metall Sin, 2007, 43(11): 1207-1210 .

Download:  PDF(722KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Using an unbalanced magnetron sputtering, hydrogen-free titanium-doped diamond-like carbon (Ti-DLC) and hydrogen-free pure diamond-like carbon (DLC) were deposited. Sputtering from titanium target and graphitic targets simultaneously to form Ti-DLC coatings, the sputtering power of titanium target was varied so the titanium concentration in the Ti-DLC coatings could be controlled from 1.9 to 34at.%. The morphology, structure were investigated by Raman、XPS、XRD and AFM. Results show that all the Ti-DLC coatings have a similar Raman spectrum with pure DLC, but dropping titanium will cause a transform from sp3 configuration to sp2 configuration. Results also show that Ti exists in a form of TiC small crystallites in the DLC structure. Compare with Ti-DLC coatings, pure DLC coating was much smoother, but for some rough base surface, titanium dropping was benefit for getting a smoother coating surface.
Key words:  unbalanced magnetron sputtering      titanium-doped diamond-like carbon      morphology      structure      
Received:  25 April 2007     
ZTFLH:  TB383  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2007/V43/I11/1207

[1]Yang S,Li X,Renevier N M,Teer D G.Surf Coat Technol, 2001;142/144:85
[2]Narayan R J.Appl Surf Sci,2005;247:217
[3]Weng K W,Chert Y C,Lin T N,Wang D Y.Thin Solid Films,2006;515:932
[4]Kulikovsky V,Bohac P,Franc F,Deineka A,Vorlicek V, Jastrabik L.Diamond Relat Mater,2001;10:1076
[5]Fu Y H,Zhu X D,He J W,Yang S C.Tribology,2003;23: 463 (付永辉,朱晓东,何家文,Yong S C.摩擦学报,2003;23:463)
[6]Siegal M P,Barbour J C,Provencio P N,Tallant D R, Friedmann T A.Appl Phys Lett,1998;73:759
[7]Siegal M P,Tallant D R,Provencio P N,Provencio D L, Overmyer D L,Simpson R L,Martine-Miranda L J.Appl Phys Lett,2000;76:3052
[8]Saitoh H.J Surf Finish Soc Jpn,2002;53:706 (斋藤秀俊.表面技术,2002;53:706)
[9]Rusli,Yoon S F,Yang H,Ahn J,Huang Q F,Zhang Q, Guo Y P,Yang C Y,Teo E J,Wee A T S,Huan A C H. Thin Solid Films,1999;355/356:174
[10]Strondl C,Carvalho N M,de Hosson J Th M,van der Kolk G J.Surf Coat Technol,2003;162:288
[11]Yang B,Huang Z H,Gao H T,Fan X J,Fu D J.Surf Coat Technol,2007;201:6808
[12]Veprek S,Haussmann M,Reiprich S.Mater Res Soc Syrup Proc,1996;86/87:394
[13]MouraeSilva C W,Bronco J R T,Cavaleiro A.Thin Solid Films,2006;515:1063
[14]Pal S K,Jiang J C,Efstathios I.Meletis Surf Coat Tech- nol,2007;201:7917
[15]Baba K,Hatada R,Tanaka Y.Surf Coat Technol,2007; 201:8362
[16]Dekempeneer E,Van Acker K,Vercammen K,Meneve J, Neerinck D,Eufinger S,Pappaert W,Sercu M,Smeets J. Surf Coat Technol,2001;142-144:669
[17]Robertson J.Prog Solid State Chem,1991;21:199
[18]Hu YW,Li L H,CaiX,Chen Q L,Chu P K,Diamond Relat Mater,2007;16:181
[19]Wang P,Wang X,Xu T,Liu W M,Zhang J Y.Thin Solid Films,2007;515:68998
[1] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[2] MA Dexin, ZHAO Yunxing, XU Weitai, WANG Fu. Effect of Gravity on Directionally Solidified Structure of Superalloys[J]. 金属学报, 2023, 59(9): 1279-1290.
[3] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[4] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[5] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[6] LIU Xingjun, WEI Zhenbang, LU Yong, HAN Jiajia, SHI Rongpei, WANG Cuiping. Progress on the Diffusion Kinetics of Novel Co-based and Nb-Si-based Superalloys[J]. 金属学报, 2023, 59(8): 969-985.
[7] LI Jingren, XIE Dongsheng, ZHANG Dongdong, XIE Hongbo, PAN Hucheng, REN Yuping, QIN Gaowu. Microstructure Evolution Mechanism of New Low-Alloyed High-Strength Mg-0.2Ce-0.2Ca Alloy During Extrusion[J]. 金属学报, 2023, 59(8): 1087-1096.
[8] CHEN Liqing, LI Xing, ZHAO Yang, WANG Shuai, FENG Yang. Overview of Research and Development of High-Manganese Damping Steel with Integrated Structure and Function[J]. 金属学报, 2023, 59(8): 1015-1026.
[9] YUAN Jianghuai, WANG Zhenyu, MA Guanshui, ZHOU Guangxue, CHENG Xiaoying, WANG Aiying. Effect of Phase-Structure Evolution on Mechanical Properties of Cr2AlC Coating[J]. 金属学报, 2023, 59(7): 961-968.
[10] SUN Rongrong, YAO Meiyi, WANG Haoyu, ZHANG Wenhuai, HU Lijuan, QIU Yunlong, LIN Xiaodong, XIE Yaoping, YANG Jian, DONG Jianxin, CHENG Guoguang. High-Temperature Steam Oxidation Behavior of Fe22Cr5Al3Mo-xY Alloy Under Simulated LOCA Condition[J]. 金属学报, 2023, 59(7): 915-925.
[11] ZHANG Deyin, HAO Xu, JIA Baorui, WU Haoyang, QIN Mingli, QU Xuanhui. Effects of Y2O3 Content on Properties of Fe-Y2O3 Nanocomposite Powders Synthesized by a Combustion-Based Route[J]. 金属学报, 2023, 59(6): 757-766.
[12] GUO Fu, DU Yihui, JI Xiaoliang, WANG Yishu. Recent Progress on Thermo-Mechanical Reliability of Sn-Based Alloys and Composite Solder for Microelectronic Interconnection[J]. 金属学报, 2023, 59(6): 744-756.
[13] WU Dongjiang, LIU Dehua, ZHANG Ziao, ZHANG Yilun, NIU Fangyong, MA Guangyi. Microstructure and Mechanical Properties of 2024 Aluminum Alloy Prepared by Wire Arc Additive Manufacturing[J]. 金属学报, 2023, 59(6): 767-776.
[14] LI Qian, LIU Kai, ZHAO Tianliang. Rust Formation Behavior and Mechanism of Q235 Carbon Steel in 5%NaCl Salt Spray Under Elastic Tensile Stress[J]. 金属学报, 2023, 59(6): 829-840.
[15] FENG Aihan, CHEN Qiang, WANG Jian, WANG Hao, QU Shoujiang, CHEN Daolun. Thermal Stability of Microstructures in Low-Density Ti2AlNb-Based Alloy Hot Rolled Plate[J]. 金属学报, 2023, 59(6): 777-786.
No Suggested Reading articles found!