| Lamellar Eutectic Growth Controlled By Solute Diffusion |
| MENG Guanghui; LIN Xin; HUANG Weidong |
| State Key Laboratory of Solidification Processing;Northwestern Polytechnical University |
|
Cite this article:
MENG Guanghui; LIN Xin; HUANG Weidong. Lamellar Eutectic Growth Controlled By Solute Diffusion. Acta Metall Sin, 2007, 43(11): 1176-1180 .
|
|
|
Abstract Based on the planar assumption, the solute boundary layer in lamellar eutectic growth in steady-state is estimated by means of modifying the conservation of mass at solid/liquid interface. It is found that the solute boundary layer along the growth direction is related to that along the solid/liquid interface. For transparent organic system CBr4-C2Cl6 of eutectic composition, the difference in average composition of the solids and that of the liquid at solid/liquid interface increases with increasing in growth velocities. The average composition in the liquid at solid/liquid interface still closes to the eutectic one as the initial composition of the alloy is apart from the eutectic point. In addition, for a fixed growth rate, the variation of ratio of the difference in average composition to the lamellar widths of the two solid phases with initial composition of the alloy is noticeably distinct.
|
|
Received: 28 March 2007
|
|
|
[1]Hunt J D.Sci Technol Adv Mater,2001;2:147 [2]Karma A,Plapp M.JOM,2004;56:28 [3]Jackson K A,Hunt J D.Trans AIME,1966;236:1129 [4]Ma D,Jie W Q.Acta Metall Sin,1996;32:791 (马东,介万奇.金属学报,1996;32:791) [5]Datye V,Langer J S.Phys Rev,1981;24B:4155 [6]Ginibre M,Akamatsu S,Faivre G.Phys Rev,1997;56E: 780 [7]Magnin P,Kurz W.In:Stefanescu D M ed,Metals Hund- book Vol.15 Casting.Metals Park,OH:ASM interna- tional,1988:119 [8]Tiller W A,Jackson K A,Rutter J W,Chalmers B.Acta Metall,1953;1:428 [9]Hunt J D.J Cryst Growth,1968;3-4:82 [10]Hunt J D,Shu-Zu Lu,In:Hurle D T.J ed.Handbook of Crystal Growth.Vol.2,Part B:Bulk Crystal Growth: Growth Mechanism and Dynamics,Amsterdam:North Holland,1994:1111 [11]Wilcox W R,Gegel L L.Acta Astronaut,1996;38:51 [12]Ma D,Li Y,Ng S C.J Cryst Growth,2000;219:300 [13]Derby B,Favier J J.Acta Metall,1983;31:1123 [14]Stocker C,Ratke L.J Cryst Growth,2000;212:324 [15]Han S H,Trivedi R.Metall Mater Trans,2000;31A:1819 [16]Karma A,Rappel W J,Fuh B C,Trivedi R.Metall Mater Trans,1998;29A:1457 [17]Kerr H W,Kurz W.Int Mater Rev,1996;41:129 [18]Liu J C,Elliott R.Acta Metall Mater,1995;43:3301 [19]Akamatsu S,Plapp M,Faivre G,Karma A.Phys Rev, 2002;66E:030501(R) [20]Series R W,Hunt J D,Jackson K A.J Cryst Growth, 1977;40:221 [21]Catalina A V,Sen S,Stefanescu D M.Metall Mater Trans, 2003;34A:383 [22]Magnin P,Trivedi R.Acta Metall Mater,1991;39:453 [23]Seetharaman V,Trivedi R.Metall Trans,1988;19A:2955! |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|