| A Coupled Model of Microsegregation and Ti--O Inclusion Precipitation During Solidification of Liquid Steel |
| ZHANG Huiquan; ZHENG Shaobo;ZHENG Qing; LIU Zili; JIANG Guochang |
| 上海大学材料学院上海市钢铁冶金重点实验室 |
|
Cite this article:
ZHANG Huiquan; ZHENG Shaobo; ZHENG Qing; LIU Zili; JIANG Guochang. A Coupled Model of Microsegregation and Ti--O Inclusion Precipitation During Solidification of Liquid Steel. Acta Metall Sin, 2006, 42(7): 745-750 .
|
|
|
Abstract ABSTRACT Basing segregation of solute elements at solid-liquid interface, a coupled model of microsegregation and Ti-O inclusion precipitation during solidification of liquid steel is established by considering finite diffusion of solute elements in both liquid and solid phases. The calculation results by this model shows that the segregation degree of solute elements is suppressed greatly due to the precipitation of Ti-O inclusions during solidification. The inclusions can be uniformly dispersed in steel by controlling due oxygen content. The number of oxides increases and their size reduces with the increasing cooling rate. The radius of the oxides only reach 0.58μm and their number and size are uniformly dispersed in steel and help to improve steel properties by controlling the condition of CSP.
|
|
Received: 21 October 2005
|
|
|
[1] Takamura J,Mizoguchi S. In: Proc 6th Int Iron and Steel Cong, Vol. 1, Tokyo: JSIJ, 1990: 591 [2] Mizoguchi S, Takamura J. In: Proc 6th Iron and Steel Cong, Vol.1, Tokyo: ISIJ, 1990: 598 [3] Sawai T, Wakoh M, Ueshima Y, Mizoguchi S. In: Proc. 6th, Iron and Steel Cong, Vol.1, Tokyo: ISIJ, 1990: 605 [4] Ogibayashi S, Yamaguchi K, Hirai M, Goto H, Yamaguchi H, Tanaka K. In: Proc 6th Iron and Steel Cong, Vol.1, Tokyo: ISIJ, 1990: 612 [5] Ueshima Y, Isobe K, Mizoguchi S, Maede H, Kajioka H. Tetsu Hagane, 1988; 74: 465 (上岛良之,矶部浩一,沟口庄三,前出弘文,尾冈博幸.铁と 钢,1988;74:465) [6] Wintz M, Bobadilla M, Lehmann J, Gaye H. ISIJ Int,1995; 35: 715 [7] Ma Z T, Janke D. ISIJ Int, 1998; 38: 46 [8] Ovtchinnikov S, Kazakov S, Janke D. Ironmaking Steelmaking, 2003; 30: 487 [9] Liu Z Z,Wei J, Cai K K.ISIJ Int, 2002; 42: 958 [10] Honma H, Matsuda S,Yamamoto K.Weld Res,1987;Suppl: 301 [11] Byun J S, Shin J H, Cho Y W, Lee D N. Acta Mater,2003; 51: 1593 [12] Yang Y, Wang F M, Song B, Luo Z T, Yang Z B. J Univ Sci Technol Beijing, 2005; 27: 540 (杨颖,王福明,宋波,罗志涛,杨占兵.北京科技大学学 报,2005;27:540) [13] Wang M T, Ma Y C, Wang L. Weld Pipe Tube, 2005; 28 (2): 15) (王茂堂,马彦昌,王丽.焊管,2005;28(2):15 [14] Ueshima Y, Mizoguchi S, Matsumiya T, Kajioka H. Metall Trans, 1986; 17B: 845 [15] Turkdogan E T. Fundamentals of Steelmaking.Cambridge:The Institute of Materials, 1996: 94 [16] The Japan Society for the Promotion of Science-the 19th Committee on Steelmaking.Steelmaking Data Sourcebook. New York: Gordon and Breach Science Publishing, 1988; 235 [17] Goto H, Miyazawa K,Yamaguchi K,Ogibayashi S,Tanaka K. ISIJ Int, 1994; 34: 414 [18] Goto H, Miyazawa K,Tanaka H K.ISIJ Int,1995;35: 708 [19] Doru M.Stefanescu,Rajesh V.Phalvikar,Pang H T, Ahuja S, Brij K. ISIJ Int, 1995; 35: 700 [20] Chen J X. Handbook of Chart Data of Steelmaking, Beijing:Metallurgical Industry Press,1984 (陈家祥.炼钢常用图表数据手册.北京:冶金工业出版社,1984) [21] Suzuki M, Yamaguchi R, Murakami K, Nakada M. ISIJ Int, 2001; 41: 247 [22] Emi H. Scand J Metall, 1975; 4: 1 [23] Goto H, Miyazawa K,Tanaka H K. ISIJ Int, 1995; 35: 286 |
| No Suggested Reading articles found! |
|
|