MICROWAVE ABSORBING CAPABILITY OF FeSiAlCr NANO-CRYSTALLINE FLAKES
Cite this article: 

. MICROWAVE ABSORBING CAPABILITY OF FeSiAlCr NANO-CRYSTALLINE FLAKES. Acta Metall Sin, 2006, 42(3): 321-324 .

Download:  PDF(211KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Nanocrystalline flakes of FeSiAlCr were synthesized by atomization process and high energy ball milling. Effect of process conditions on microstructure, morphology and microwave electromagnetic characteristics of FeSiAlCr particles were investigated. Results show that flaky morphology and nanocrystalline microstructure were gained by process of high energy ball milling. Thus, microwave permeability were improved remarkably and permittivity were controlled effectively. Effect of sequent annealing was also discussed and it was found that microwave electromagnetic performances were improved further. Microwave absorbing ability of coating layer made of the nanocrystalline FeSiAlCr flakes proved that the materials can be applied in suppression of electromagnetic interference or microwave absorption.
Key words:  nanocrystalline      FeSiAlCr alloy      complex permeability      microwave absorber      high energy ball milling      
Received:  09 June 2005     
ZTFLH:  TM277  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2006/V42/I3/321

[1] Sugimoto S, Maeda T, Book D, Kagotani T, Sato R. J Alloys Compd, 2002; 330-332: 301
[2] Matsumoto M, Miyata Y. IEEE Trans Magn, 1997; 33: 4459
[3] Walser R M, Win W, Valanju P M. IEEE Trans Magn, 1998; 34: 1390
[4] Herzer G. IEEE Trans Magn, 1990; 26: 1397
[5] Yang D S. J Low Temp Phys, 1997; 19: 299 (杨东升.低温物理学报, 1997;19:299)
[6] Thoumire O, Atmani H. J Magn Magn Mater, 1999; 196-197: 346
[7] Liu T, Pu Y X. Chin Sci Bull, 1995; 40: 666 (刘 涛,蒲玉写.科学通报, 1995;40:666)O
[1] HUANG Ding, QIAO Yanxin, YANG Lanlan, WANG Jinlong, CHEN Minghui, ZHU Shenglong, WANG Fuhui. Effect of Shot Peening of Substrate Surface on Cyclic Oxidation Behavior of Sputtered Nanocrystalline Coating[J]. 金属学报, 2023, 59(5): 668-678.
[2] WANG Yihan, YUAN Yuan, YU Jiabin, WU Honghui, WU Yuan, JIANG Suihe, LIU Xiongjun, WANG Hui, LU Zhaoping. Design for Thermal Stability of Nanocrystalline Alloys Based on High-Entropy Effects[J]. 金属学报, 2021, 57(4): 403-412.
[3] Xiubing LIANG, Jianwen FAN, Zhibin ZHANG, Yongxiong CHEN. Microstructure and Corrosion Properties of Aluminum Base Amorphous and Nanocrystalline Composite Coating[J]. 金属学报, 2018, 54(8): 1193-1203.
[4] Feng LIU, Linke HUANG, Yuzeng CHEN. Concurrence of Phase Transition and Grain Growth in Nanocrystalline Metallic Materials[J]. 金属学报, 2018, 54(11): 1525-1536.
[5] Yaoxiang GENG,Xin LIN,Jianbing QIANG,Yingmin WANG,Chuang DONG. Dual-Cluster Characteristic and Composition Optimization of Finemet Soft Magnetic Nanocrystalline Alloys[J]. 金属学报, 2017, 53(7): 833-841.
[6] Yufeng ZHENG,Yuanhao WU. Revolutionizing Metallic Biomaterials[J]. 金属学报, 2017, 53(3): 257-297.
[7] Jiaojiao DU,Guojian LI,Qiang WANG,Yonghui MA,Huimin WANG,Mengmeng LI. GROWTH MODE EVOLUTION AND SUBSEQUENT MAGNETIC PROPERTIES OF Fe FILMS WITH DIFFERENT GRAIN SIZES UNDER A HIGH MAGNETIC FIELD[J]. 金属学报, 2015, 51(7): 799-806.
[8] NI Song, LIAO Xiaozhou, ZHU Yuntian. EFFECT OF SEVERE PLASTIC DEFORMATION ON THE STRUCTURE AND MECHANICAL PROPERTIES OF BULK NANOCRYSTALLINE METALS[J]. 金属学报, 2014, 50(2): 156-168.
[9] PENG Xiao, WANG Fuhui. HIGH TEMPERATURE CORROSION OF NANO-CRYSTALLINE METALLIC MATERIALS[J]. 金属学报, 2014, 50(2): 202-211.
[10] LIU Li, LI Ying, WANG Fuhui. ELECTROCHEMICAL CORROSION BEHAVIOR OF NANOCRYSTALLIZED MATERIALS: GROWTH OF PASSIVE FILM AND LOCAL PITTING CORROSION[J]. 金属学报, 2014, 50(2): 212-218.
[11] LI Xiaoyan. ATOMISTIC SIMULATIONS OF BAUSCHINGER EFFECT IN NANOCRYSTALLINE ALUMINUM THIN FILMS[J]. 金属学报, 2014, 50(2): 219-225.
[12] ZHOU Xiaowei,SHEN Yifu. CORROSION BEHAVIOR AND EIS STUDY OF NANOCRYSTALLINE Ni-CeO2 COATINGS IN AN ACID NaCl SOLUTION[J]. 金属学报, 2013, 49(9): 1121-1130.
[13] WU Yan, ZONG Yaping,ZHANG Xiangang. MICROSTRUCTURE EVOLUTION OF NANOCRYSTALLINE AZ31 MAGNESIUM ALLOY BY PHASE FIELD SIMULATION[J]. 金属学报, 2013, 49(7): 789-796.
[14] CHAO Yuesheng, WANG Li, ZHANG Yanhui, ZHU Hanxian, LUO Liping. EFFECT OF LOW-TEMPERATURE VACUUM ANNEALING ON THE MAGNETIC PULSED AMORPHOUS Fe52Co34Hf7B6Cu1 ALLOY[J]. 金属学报, 2012, 48(6): 749-752.
[15] LIU Rongming, YUE Ming, ZHANG Dongtao,Liu Weiqiang, ZHANG Jiuxing. PREPARATION, STRUCTURE AND MAGNETIC PROPERTIES OF SmCo5 NANOPARTICLES AND NANOFLAKES[J]. 金属学报, 2012, 48(4): 475-479.
No Suggested Reading articles found!