| THERMAL FATIGUE BEHAVIOR OF NICKEL BASE SUPERALLOY K445 |
| ;; |
|
Cite this article:
. THERMAL FATIGUE BEHAVIOR OF NICKEL BASE SUPERALLOY K445. Acta Metall Sin, 2006, 42(10): 1056-1060 .
|
|
|
Abstract A study of thermal fatigue (TF) behavior of cast nickel-base superalloy K445 was conducted between the temperatures ranging from 800℃ to 900℃ and RT, using plate specimens notched to induce crack initiation. Conventional optical microscopy (OM) and scanning electron microscopy (SEM) examinations were conducted to investigate the damage mechanisms of thermal fatigue. Almost all the primary fatigue cracks at elevated temperatures propagate intergranularly and the secondary crack is transgranular. At 800℃, coarse MC carbides either at grain boundaries or within the grain interior, as well as decohesion of MC/matrix interface, are the preferential sites of crack initiation and propagation. At 900℃, crack propagation is an oxidation-dominant and carbide-assisted process. Stress assisted grain boundary oxygen (SAGBO) embrittlement is the principle mechanism of the environmental degradation to the alloy at the crack-tip region.
|
|
Received: 04 April 2006
|
|
|
[1]Varin J D.In:Sims C T,Hagel W C eds,The Superalloys,New York:John Wiley & Sons,1972:242 [2]Blümm M,Demestral B,Eggeler G,Réza(?)-Aria F.Scr Metall Mater,1995;33:719 [3]Felberbaum L,Voisey K, G(?)umann M,Viguier B,Mortensen A.Mater Sci Eng,2001;A299:152 [4]Li Z J,Zhou L Z,Guo J T,Yao J.J Mater Eng,2005;(8):24(李志军,周兰章,郭建亭,姚俊.材料工程,2005;(8):24) [5]Yuan F H,Sun X F,Guan H R,Hu Z Q.J Mater Eng,2001;(Suppl):22 ??(袁福河,孙晓峰,管恒荣,胡壮麒.材料工程,2001;(增刊):22) [6]Woodford D A,Mowbray D F.Mater Sci Eng,1974;16:5 [7]Glenny E,Taylor T A.J Inst Met,1959-1960;88:449 [8]Bhattachar V S.Int J Fatigue,1995;17:407 [9]Reuchet J,Rémy L.Mater Sci Eng,1983;58:33 [10]He L Z,Zheng Q,Sun X F,Guan H R,Hu Z Q,Tieu A K,Lu C,Zhu H T.Mater Sci Eng,2005;A397:297 [11]Chen Q Z,Jones C N,Knowles D M.Mater Sci Eng,2004;A385:402 [12]Kaufman M.In:Gell M,Kortovich C S,Bricknell R H,Kent W B,Radavich J F eds,Superalloy 1984,Warrendale PA:AIME,1984:43 [13]Elliott R O,Kempter C P.J Phys Chem,1958;62:630 [14]Brandes E A.Smithells Metals Reference Book.6th Edition,London:Butterworths,1983:14 [15]Reuchet J,Pémy L.Mater Sci Eng,1983;58:19 [16]Florren S,Kane R.Metall Trans,1979;10A:1745 [17]Li M S.High Temperature Corrosion of Metals.Beijing:Metallurgical Industry Press,2001:349(李美栓.金属的高温腐蚀.北京:冶金工业出版社,2001:349) [18]Kang B,Liu X B,Cisloiu C,Chang K M.Mater Sci Eng,2003;A347:205w |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|