					Cite this article:
						|  |  
    					|  |  
    					| FULL-ELECTRON CALCULATION OF α-LaNi5H0.5 and β-LaNi5H3 |  
						| QI Xinhua; GAO Tao; CHEN Bo |  
						| Institute of Atomic and Molecular Physics; Sichuan University; Chengdu 610065 |  
						|  |  
					
			      QI Xinhua; GAO Tao; CHEN Bo. FULL-ELECTRON CALCULATION OF α-LaNi5H0.5 and β-LaNi5H3. Acta Metall Sin, 2005, 41(9): 910-916       .	
				 
					
						| 
								
									|  
          
          
            
              
				
												  
													
													    |  |  
														| Abstract  Based on the generalized gradient approximation (GGA) of density function and the full-potential linearized augmented plane wave (FLAPW) method, the equilibrium structure and density of states were calculated for the primary solid solution phase α-LaN5H0.5 and the intermediate
phase β-LaNi5H3. In the α-phase region, 12n site is the most stable position in five nonequivalent interstices; with increasing H atoms the cell parameter a axis increases, while the c axis is constant. In the α→β region, with increasing H atoms a large increase in the a$ axis and a relatively small increase in the c axis are concluded. The charge density and density of states are also calculated for the intermediate phase. |  
															| Received:  20 January 2005 |  
															|  |  
            
									            
									               
																												  
															| [1] Flanagan T B, Wulff C A, Bowerman B S. J Solid State Chem, 1980; 34: 215 [2] Murray J J, Post M L, Taylor J B. J Less-Common Met, 1981; 80: 211
 [3] Feng Z K, Yang H X, Jiao Y L, Ma Z Q. Rare Met Mater Eng, 1990; (1): 59 (冯治库,杨宏秀,焦玉琏,马忠乾.稀有金属材料与工程,1990; (1):59)
 [4] Fischer P, Furrer A, Busch G, Schlapbach L. Phys Acta, 1977; 50: 421
 [5] Soubeyroux J L, Percheron-Guegan A, Achard J C. J Less-Common Met, 1987; 129: 181
 [6] Kisi E H, Gray E M A, Kennedy S J. J Alloys Compd, 1994; 216: 213
 [7] Hempelmann R, Richter D, Eckold G. J Less-Common Met, 1984; 104: 1
 [8] Nakamura H, Nguyen-Manh D, Pettifor D G. J Alloys Compd, 1998; 281: 81
 [9] Tatsumi K, Tanaka I, Inui H, Tanaka K, Yamaguchi M, Adachi H. Phys Rev, 2001; 64B: 184105
 [10] Nomura K, Uruno H, Shinozuka H, Suda S, Ono S. J LessCommon Met, 1985; 107: 221
 [11] Akiba E, Nomura K, Ono S. J Less-Common Met, 1987; 129: 159
 [12] Ono S, Nomura K, Akiba E. J Leas-Common Met, 1985; 113: 113
 [13] Akiba E, Hayakawa H, Ishido Y, Nomura K. Phys Chem, 1989; 163: 291
 [14] Van Vucht J H N, Kuipers F A, Bruning H C M.Philips Res Rep,1970;25:133
 [15] Blaha P,Schwarz K, Madsen G K H, Kvasnicka D, Luitz J. Computer Code WIEN2K, An Augmented Plane Wave Plus Local Orbital Program for Calculating Crystal Properties, Vienna, Austria: Vienna University of Technology, 2001
 [16] Westlake D G. J Less-Common Met, 1983; 90: 251
 [17] Qi X H, Gao T, Zhu Z H. J Atom Mol Phys, 2004; 21: 366 (齐新华,高 涛,朱正和.原子与分子物理学报,2004;21: 366)
 [18] Guo J, Wei W L, Ma S Y. Acta Metall Sin, 2003; 39: 10 (郭进,韦文楼,马树元.金属学报, 2003;39:10)w
 |  
             
								                
															
																| 
																																																																									
																				| No Suggested Reading articles found! |  |  
             
												
											    	
											        	|  | Viewed |  
											        	|  |  |  
												        |  | Full text 
 | 
 
 |  
												        |  |  |  
												        |  | Abstract 
 | 
 |  
												        |  |  |  
												        |  | Cited |  |  
												        |  |  |  |  
													    |  | Shared |  |  
													    |  |  |  |  
													    |  | Discussed |  |  |  |  |