| The Role of Sn Substitution for Si And B to Enhance the Amorphization of Mechanically-Milled Ti50Ni22Cu18Al4Si4B2 Alloy |
| ZHANG Laichang; SHEN Zhiqi; XU Jian |
| Shenyang National Laboratory for Materials Science; Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110016 |
|
Cite this article:
ZHANG Laichang; SHEN Zhiqi; XU Jian. The Role of Sn Substitution for Si And B to Enhance the Amorphization of Mechanically-Milled Ti50Ni22Cu18Al4Si4B2 Alloy. Acta Metall Sin, 2004, 40(9): 981-986 .
|
|
|
Abstract Elements Si and B in the
Ti50Ni22Cu18Al4Si4B2
alloy are substituted with Sn to
form the Ti50Ni22Cu18Al4Snx(Si0.67B0.33)6-x (x=0,3,6) series
alloys. In all cases, mechanical
milling of the prealloyed fragments
results in the amorphization of the alloys. With increasing
the Sn content in the alloys, the fraction of residual α-Ti
crystallites in the final milled product
was reduced. For the Ti50Ni22Cu18Al4Sn6
alloy, in which the Si and B are completely replaced
with Sn, the nearly complete amorphization is achievable.
A single amorphous phase, similar to the melt-quenched glass,
formed in the milled alloy. Such a ball-milled glassy alloy
exhibits a large supercooled liquid region about 66 K.
|
|
Received: 05 April 2004
|
|
|
[1] Inoue A, Kimura H M, Masumoto T, Suryanarayana C,Hoshi A. J Appl Phys, 1980; 51: 5475 [2] Inoue A, Amiya K, Katsuya A, Masumoto T. Mater TransJIM, 1995; 36: 858 [3] Zhang T, Inoue A. Mater Sci Eng, 2001; A304-306: 771 [4] Zhang T, Inoue A. Mater Trans JIM, 1999; 40: 301 [5] Kim Y C, Kim W T, Kim D H. Mater Trans, 2002; 43:1243 [6] Nishiyama N, Inoue A. Mater Trans JIM, 1997; 38: 464 [7] Inoue A, Zhang T. Mater Trans JIM, 1996; 37: 185 [8] Johnson W L. Mater Sci Forum, 1996; 225-227: 35 [9] Kawamura Y, Kato H, Inoue A, Masumoto T. Appl PhysLett, 1995; 67: 2008 [10] Kawamura Y, Kato H, Inoue A, Masumoto T. Int J Powder Metall, 1997; 33: 50 [11] Sordelet D J, Rozhkova E, Huang P, Wheelock P B, BesserM F, Kramer M J, Calvo-Dahlborg M, Dahlborg U. JMater Res, 2002; 17: 186 [12] Itoi T, Takamizawa T, Kawamura Y, Inoue A. Scr Mater,2001; 45: 1131 [13] Ishihara S, Zhang W, Inoue A. Scr Mater, 2002; 47: 231 [14] Lee M H, Bae D H, Kim W T, Kim D H, Rozhkova E,Wheelock P B, Sordelet D J. J Non-Gryst Solids, 2003;315: 89 [15] Robertson J, Im J T, Karaman I, Hartwig K T, AndersonI E. J Non-Cryst Solids, 2003; 317: 144 [16] Karaman I, Robertson J, Im J T, Mathaudhu S N, Luo ZP, Hartwig K T. Metall Mater Trans, 2004; 35A: 247 [17] Zhang L G, Xu J, Ma E. J Mater Res, 2002; 17: 1743 [18] Zhang T, Inoue A. Mater Trans JIM, 1998; 39: 1001 [19] Kim Y C, Yi S, Kim W.T, Kim D H. Mater Sci Forum,2001; 360-362: 67 [20] Kim Y C, Yi S, Kim W T, Kim D H. Mater Res Soc SympProc, 2001; 644: L4. 9. 1 [21] Zhang L C, Xu J. Mater Sci Forum, 2002; 386-388: 47 [22] Sagel A, Wunderlich R K, Perepezko J H, Fecht H J. ApplPhys Lett, 1997; 70: 580 [23] Zhang L C, Shen Z Q, Xu J. J Mater Res, 2003; 18: 2141 [24] Chen L C, Spaepen F. J Appl Phys, 1991; 69: 679 [25] Schwarz R B, Petrich R R, Saw C K. J Non-Cryst Solids,1985; 76: 281 [26] Eckert J, Schultz L, Urban K. J Non-Cryst Solids, 1991;127: 90 [27] Politis C, Johnson W L. J Appl Phys, 1986; 60: 1147 [28] O'Brien J W, Dunlap R A, Dahn J R. J Alloys Compd,.2003; 353: 65 |