| Analysis on Internal Oxidation Technology of Al in Cu—Al Pre--Alloyed Powders |
| CHEN Sihong; LÜ Manqi; ZHANG Jingdang; DONG Jiasheng;YANG Ke |
| Intstitute of Metal Research; The Chinese Academy of Sciences |
|
Cite this article:
CHEN Sihong; LÜ Manqi; ZHANG Jingdang; DONG Jiasheng; YANG Ke. Analysis on Internal Oxidation Technology of Al in Cu—Al Pre--Alloyed Powders. Acta Metall Sin, 2004, 40(3): 314-318 .
|
|
|
Abstract The ferrite and austenite stainless steels containing a suitable amount of Cu may be of antibacterial ability after a special antibacterial treatment. The distribution and appearance of the precipitates appeared in the Cu--contained stainless steels were studied with TEM. The results of antibacterial examination show that Cu--contained ferrite and austenite stainless steels have broad--spectrum antibacterial properties. By using bio--TEM, a obvious change of the bacterium appearance on the surface of antibacterial stainless steel is observed and a lot of bacteria enchyma leaks out.
|
|
Received: 24 March 2003
|
|
|
[1] Li B Z. New Chem Mater, 2000; 26(6) :8(李毕忠.化工新型材料,2000;26(6) :8) [2] Huang Z. J Mater Rev, 1999; 13(2) :35(黄占杰.材料导报,1999;13(2) :3) [3] Yamamoto M. Spec Steels (Jpn), 1999; 48(6) :24 [4] Nakamura S, Ookubo N, Miyakusu K, Hasegawa M. Nisshin Steel, 1997; 76:48 [5] Ookubo N, Nakamura S, Yamamoto M, Miyakusu K, Hasegawa M. Nisshin Steel, 1998; 77:69 [6] Yokota T, Tochihara M, K Takao. Kawasaki Steel, 1998; 30:121 [7] Toyokihara C, Nakamura S, Miyakusu K. CAMP-ISIJ, 1999; 12:1179 [8] Suzuki S, Nakamura S Ookubo N, Hasegawa M, Miyakusu K. CAMP-ISIJ, 1999; 12:518 [9] Chen SH, Lu M Q, Yang K, Zhang J D. Chinese Patent, 0214568. 0(陈四红,吕曼祺,杨柯,张敬党.中国发明专利,0214568. 0) [10] Yamamoto M. Grocery Mach, 1997; 11:99 [11] Kang Z Y, Li R Z, Che C B. J Harbin Univ Sci Technol, 1995; 19:103(康湛莹,李瑞增,车城斌.哈尔滨科学技术大学学报,1995;19:103) [12] Ellis G P, Luscombe D K. Prog Med Chem, 1990; 31:351 [13] Ritchie J A. Lett Appl Microbiol, 1990; 11:152 [14] Feng Q L, Kim T N, Wu J, Park E S, Kim J O, Lira D Y, Cui F Z. Thin Solid Films, 1998; 335:214? |
| No Suggested Reading articles found! |
|
|