| Three--Dimensional Figure of Normal Stress and Shear Stress at One Point and Its Application in Analyzing Metal Forming Process |
| HE Zhubin; WANG Zhongren; YUAN Shijian |
| School of Materials Science and Engineering; Harbin Institute of Technology |
|
Cite this article:
HE Zhubin; WANG Zhongren; YUAN Shijian. Three--Dimensional Figure of Normal Stress and Shear Stress at One Point and Its Application in Analyzing Metal Forming Process. Acta Metall Sin, 2004, 40(3): 319-325 .
|
|
|
Abstract A three--dimensional figure of normal stress and shear stress of one stress state was given, and the corresponding relationship of the figure with deformation type was analyzed.The figures can be divided into three main types, which refer to compression, plain strain, and tension, respectively.
In addition, the stress--strain of typical points in simple tension, drawing, and extrusion was successfully analyzed by the figures.
|
|
Received: 03 March 2003
|
|
|
[1] Hagen H, Ebert A, van Lengen R H, Scheuermann G. International Conference on Informatics-10 Years Back, 10 Years Ahead, Dagstuhl, Germany, 2000 [2] Wang Z R, Dai K. Acta Metall Sin, 2000; 36:46(王仲仁,戴昆.金属学报,2000;36:46) [3] Kun Dai, Wang Z R. J Mater Proc Technol, 2000; 102:174 [4] Wang Z R. Fundamental of Plastic Working Mechanics. Beijing: National Defence Industry Press, 1989:127(王仲仁.塑性加工力学基础.北京:国防工业出版社,1989:127)U |