| Evaluation of Tensile Strength of BT25Y Titanium Alloy in Terms of Equivalents |
| YANG Weiguo 1); WANG Qingjiang 2);ZHANG Caibei 1); LIU Yuyin 2) |
| 1) Science Department; Northeastern University; Shenyang 110006; 2) Institute of Metal Research; The Chinese Academy of Sciences;Shenyang 110016 |
|
Cite this article:
YANG Weiguo; WANG Qingjiang; ZHANG Caibei; LIU Yuyin . Evaluation of Tensile Strength of BT25Y Titanium Alloy in Terms of Equivalents. Acta Metall Sin, 2004, 40(2): 155-158 .
|
|
|
Abstract The tensile strengths of the duplex microstructural
BT25Y titanium alloys with different contents
of Al, W, and Mo have been measured
at room and high temperatures. According to Kolachev' formula, the
equivalent formulae of yield strength and ultimate tensile strength
were derived with the experimental results. The calculated
strengths from these equivalent formulae also accord with the
experimental values of BT25Y titanium alloys with widmanstatten
microstructure at variant temperatures.
|
|
Received: 24 February 2003
|
|
|
[1] Kolachev B A, Ilyin A A, Volodin V A, Ryndenkov D V. In: Gorynin I V, Ushkov S S, eds., Titanium'99: Science and Technology, Proc 9th World Conf on Titanium Science and Technology, Vol. 1, St. Petersburg, Russia: Central Research Institute of Structural Materials, 2000: 53 [2] Hui S X, Zhang Z, Xiao J S, Yuan G S. Rare Met, 1999; 23: 125(惠松骁,张翥,萧今声,袁冠森.稀有金属,1999;23:125) [3] Flower H M. Mater Sci Technol, 1990; 6: 1082 [4] Greenfield M A, Kuhlken N, Margolin H. Metall Trans, 1971; 2: 610 [5] Lu G, Zhang Z, Hui S X, Li Z K, Chen Z Q, He S L. Acta Metall Sin, 2002; 38(Suppl.): S206(路纲,张翥,惠松骁,李宗科,陈占乾,何书林.金属学报,2002;38(增刊):S206) [6] Ltjering G. Mater Sci Eng, 1998; A243: 32 [7] Albrecht J, Ltjering G. In: Gorynin I V, Ushkov S S, eds., Titanium'99: Science and Technology, Proc 9th World Conf on Titanium Science and Technology, Vol. 1, St. Petersburg, Russia: Central Research Institute of Structural Materials, 2000: 363 |