| Micro-Simulation of Crack Tip Plastic Zone and Dislocation-Free Zone |
| QIAN Caifu; JIANG Zhongjun; CHEN Ping; DUAN Chenghong; CUI Wenyong |
| Department of Process Equipment and Control Engineering; Beijing University of Chemical Technology; Beijing 100029 |
|
Cite this article:
QIAN Caifu; JIANG Zhongjun; CHEN Ping; DUAN Chenghong; CUI Wenyong. Micro-Simulation of Crack Tip Plastic Zone and Dislocation-Free Zone. Acta Metall Sin, 2004, 40(2): 159-162 .
|
|
|
Abstract Edge dislocation emissions from Mode I, Mode II and mixed-mode crack
tips along multiple inclined slip planes are simulated, and plastic
zones as well as dislocation--free zones are obtained. It is found
that the shape of the Mode II plastic zone is quite different from that
obtained based on von Mises yielding criterion and consists of three parts
in which the biggest one locates in front of the crack tip. For Mode I
crack, however, a similar plastic zone is obtained. Under the same
magnitudes of applied stress, the plastic zone of Mode II crack is
much larger than that of Mode I crack, and the plastic zone of a
mixed--mode crack is mainly affected by the Mode II component.
Dislocation--free zones exist around all types of crack tips,
which have similar shapes as the corresponding plastic zones.
|
|
Received: 24 February 2003
|
|
|
[1] Ohr S M. Mater Sci Eng, 1985; 72: 1 [2] Chiao Y H, Clarke D R. Acta Metall, 1989; 37: 203 [3] Zielinski W, Lii M J, Gerberich W W. Acta Metall Mater, 1992; 40: 2861 [4] Marsh P G, Zielinski W, Huang H, Gerbrich W W. Acta Metall Mater, 1992; 40: 2883 [5] Li C, Zhao H, Zhan Z, Zhou H. Eng Fract Mech, 1992; 43: 1009 [6] Chia K Y, Burns S J. Scr Metall, 1984; 18: 467 [7] Fu R, Long Q Y, Zhang T Y, Lung C W. J Phys, 1989; 22D: 991 [8] Foeke T, Gerberich W W. Scr Metall Mater, 1990; 24: 553 [9] Bilby B A, Cottrell A H, Swinden K H. Proc R Soc London, 1963; 272: 304 [10] Chang S J, Ohr S M. J Appl Phys, 1981; 52: 7174 [11] Dai S H, Li J C M. Scr Metall, 1982; 16: 183 [12] Majumdar B S, Burns S J. Acta Metall, 1981; 29: 579 [13] Zhao R H, Dai S H, Li J C M. Int J Fract, 1985; 29: 3 [14] Zhao R H, Li J C M. J Eng Mater Technol, 1985; 107A: 277 [15] Zhao R H, Li J C M. J Appl Phys, 1985; 58B: 4117 [16] Pippan R. Scr Metall, 1989; 23: 1575 [17] Li J, Li J C M. Mater Sci Eng, 1990; 129A: 167 [18] Li J, Li J C M. Mater Sci Eng, 1990; 129A: 175 [19] Yokobori A T Jr, Isogai T. Yokobori T. Acta Metall Mater, 1993; 41: 1405 [20] Loyola de Oliveira M A, Michot G. Mater Sci Eng, 1994; 176A: 139 [21] Lakshmanan V, Li J C M. Mater Sci Eng, 1988: 104A: 95 [22] Qian C F, Li J C M. Mech Mater, 1996; 24A: 1 [23] Qian C F, Li J C M. Mech Mater, 1996; 24A: 11 [24] Chen Q Z, Chu W Y, Hsiao C M. Acta Metall Mater. 1995; 43: 4371 [25] Qiao L J, Mao X, Chen Q Z. Metall Mater Trans, 1995; 26A: 1461 [26] Zhang Y, Wang Y B, Chu W Y. Scr Metall Mater, 1994; 31: 279 [27] Chen Q Z, Gao K W, Zhang Y, Chu W Y. Fatigue Fract Eng Mater Struct, 1998; 21: 1415 [28] Qian C F, Qiao L J, Chu W Y. Sci Chin, 2000; 43E: 421 [29] He Q Z, Li Z N. Engineering Fracture Mechanics. Beijing: Beijing University of Aeronautic and Astronautic Press, 1993: 47(何庆芝,郦正能.工程断裂力学.北京:北京航空航天大学出版社,1993:47) [30] Ha K F. Physical Basis for Fracture. Beijing: Science Press, 2000: 150(哈宽富.断裂物理基础.北京:科学出版社,2000:150) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|