CONSISTENCY(OR SIMILARITY) OF THERMODYNAMIC PROPERTIES OF METALLURGICAL MELTS WITH THEIR PHASE DIAGRAMS
ZHANG Jian(Metallurgical Engineering School; University of Science and Technology Beijing; Beijing 100083)
Cite this article: 

ZHANG Jian(Metallurgical Engineering School; University of Science and Technology Beijing; Beijing 100083). CONSISTENCY(OR SIMILARITY) OF THERMODYNAMIC PROPERTIES OF METALLURGICAL MELTS WITH THEIR PHASE DIAGRAMS. Acta Metall Sin, 1998, 34(7): 742-752.

Download:  PDF(952KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  After combining investigation of thermodynamic properties of binary metallic melts, molten slags, molten salts and mattes with their phase diagrams, it has been found that in case of identical or similar phase diagrams, the calculating models of mass action concentrations of different metallurgical melts are identical (consistency) in the major cases, and similar (similarity)in the minor cases.
Key words:  metallurgical melt      molten slag      molten salt      matte      phase diagram      thermodynamics     
Received:  18 July 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I7/742

1 Hultgren R, Desai P D, Hawkins D T, Gleiser M, Kelley K K. Selected Values of the ThermodynamicProperties of Binary Alloys. Metals Park, Ohio: ASM, 1973: 241, 85
2 Proc 4th Int Conf on Molten Slags and Fluxes, 8 - 11, June, 1992, The Iron and Steel Institute of Japan,Sendai, Japan
3 邹元曦.邹元曦论文集上海:中国科学院上海冶金研究所,1988(Zou Yuanxi. Collected Wowhs of Zou Yuanxi Shanghai: Shanghai Metallurgical Institute, The Chinese Academy of Sciences,1988)
4 魏寿昆.活度在冶金物理化学中的应用北京:中国工业出版社,1964(We Shouku. Applications of Activity to the Physical Chemistry of Metallargicla Processes.Beijing:Press of chnese Industry,1964)
5 张鉴.金属学报,1998;34:75(Zhang Jian. Acta Metall Sin, 1998; 34: 75)
6 张鉴.炉外精炼的理论与实践北京:冶金工业出版社,1993:103(Zhang Jian. Theory and Practice of Secondary Refining. Beijing:The Metallurgical Industry Press,1993:103)
7 Zhang Jian. Proc Int Ferrous Metallurgy Professor Seminar 8-10, November, 1986, Beijing, Beijing Universityof Iron and Steel Technology, 1986: 4 - 1
8 张鉴.金属学报,1997;33:515 (Zhang Jian. Acta Metall Sin, 1997; 33: 515)
9 张鉴.中国有色金属学报,1997;7(3):38(Zhang Jian.Chin J onfer Met,1997 7(3):38)
10 古川武,加藤 一铁 钢,1975;61:3060(Furukawa T, Kato E. Tetsu Hapane, 1975 61: 3060)
11 张鉴.北京科技大学学报,1989;11:208(Zhang Jian.J Univ Sci Technol Beijing, 1989; 11: 208)
12 Yamapuchi S, Imai A, Goto K S Scan J Metall; 1982;(11): 263
13 Rego D N, Siporth G K, Philbrook W O、 Metall Trans, 1985; 16B: 313
14 月桥文孝,佐野信雄铁上钢,1985;71:815(Tsukihashi F; Sano N. Tetsu Hagane, 1985; 71: 815)
15 Wang Zhichang, Tian Yanwen, Yu Hualongt Zhou Jiankang. Metall Trans, 1992; 23B: 666
16 Koh J, Itagaki K. Trans Jpn Inst Met, 1984 25: 367
17 张鉴中国有色金属学报,1997;7(4):30(Zhang Jian. Chin J Nonfer Met, 1997; 7(4): 30)
18 成国光,张鉴北京科技大学学报,19942 16(1):10(Cheng Guoguang, Zhang Jian. J Univ Sci Technol Beijing; 1994; 16(1): 10)
19 Karatwa I, Thompson W T. Can Metall Q, 1986; 25: 307
20 成国光,张鉴.上海金属,1993; 15(6): 22 (Cheng Gujoguang,Zhang Jian.Shanghai Met;1993; 15(6):22)
21 Rao D P, Gaskel D R. Metall Trans, 1981; 12B: 311
22 Zhang Jian. J Univ Sci Technol Beijing, 1994; (1-2): 22
23 Eric R H. Metall Trans, 1993; 24B: 301
24 Chipman J. Discuss Faraday Soc, 1948; (4): 23
25 Zhang Jian. Trans Noafer Met Soc Chin, 1995; 5(2): 16
26 张鉴.二元氧化物固清体的作用浓度计算模型见:庆祝林宗彩教授八十寿辰论文集,北京:冶金工业出版社, 1996:110 (Zhang Jian. Calculating Models of Mass Action Concentrations for, Binary Oxide Solid Solutions.In: Proceedings for Congratulation of the 80th Birthdny of Professor Lin Zongcai, Beijing: The Metallurgical Industry Press, 1996: 110)
27 Davis B R, Thompson W T. Can Metall Q, 1995; 34: 347
28 Davis B R, Thompson W T. J Electrochem Soc, 1992; 139: 869N
[1] ZHANG Yuexin, WANG Jujin, YANG Wen, ZHANG Lifeng. Effect of Cooling Rate on the Evolution of Nonmetallic Inclusions in a Pipeline Steel[J]. 金属学报, 2023, 59(12): 1603-1612.
[2] GAO Jianbao, LI Zhicheng, LIU Jia, ZHANG Jinliang, SONG Bo, ZHANG Lijun. Current Situation and Prospect of Computationally Assisted Design in High-Performance Additive Manufactured Aluminum Alloys: A Review[J]. 金属学报, 2023, 59(1): 87-105.
[3] LIU Feng, WANG Tianle. Precipitation Modeling via the Synergy of Thermodynamics and Kinetics[J]. 金属学报, 2021, 57(1): 55-70.
[4] GAO Xiang, ZHANG Guikai, XIANG Xin, LUO Lizhu, WANG Xiaolin. Effects of Alloying Elements on the Adsorption of Oxygen on V(110) Surfaces: A First-Principles Study[J]. 金属学报, 2020, 56(6): 919-928.
[5] WANG Zumin,ZHANG An,CHEN Yuanyuan,HUANG Yuan,WANG Jiangyong. Research Progress on Fundamentals and Applications of Metal-Induced Crystallization[J]. 金属学报, 2020, 56(1): 66-82.
[6] Chengming ZHENG, Qingchao TIAN. Effect of Alloy Elements on Oxidation Behavior of Piercing Plug Steel[J]. 金属学报, 2019, 55(4): 427-435.
[7] Liheng LIU,Chunshan CHE,Gang KONG,Jintang LU,Shuanghong ZHANG. DESTABILIZATION MECHANISM OF Fe-Al INHIBITION LAYER IN Zn-0.2%Al HOT-DIP GALVANIZING COATING AND RELATED THERMODYNAMIC EVALUATION[J]. 金属学报, 2016, 52(5): 614-624.
[8] Feng LIU, Kang WANG. DISCUSSIONS ON THE CORRELATION BETWEEN THERMODYNAMICS AND KINETICS DURING THE PHASE TRANSFORMATIONS IN THE TMCP OF LOW-ALLOY STEELS[J]. 金属学报, 2016, 52(10): 1326-1332.
[9] Tao LIU,Jiasheng DONG,Guang XIE,Yisheng WANG,Hui LI,Zhijun LI,Xingtai ZHOU,Langhong LOU. CORROSION BEHAVIOR OF GH3535 SUPERALLOY IN FLiNaK MOLTEN SALT[J]. 金属学报, 2015, 51(9): 1059-1066.
[10] Chuan HONG,Yunming GAO,Chuanghuang YANG,Zhibo TONG. ELECTROCHEMICAL BEHAVIOR OF Ni2+ IN SiO2-CaO-MgO-Al2O3 MOLTEN SLAG AT 1673 K[J]. 金属学报, 2015, 51(8): 1001-1009.
[11] XIE Jun, YU Jinjiang, SUN Xiaofeng, JIN Tao, SUN Yuan. CARBIDE EVOLUTION BEHAVIOR OF K416B AS-CAST Ni-BASED SUPERALLOY WITH HIGH W CONTENT DURING HIGH TEMPERATURE CREEP[J]. 金属学报, 2015, 51(4): 458-464.
[12] WU Changjun, ZHU Chenlu, SU Xuping, LIU Ya, PENG Haoping, WANG Jianhua. THERMODYNAMICAL AND KINETIC INVESTIGA-TION OF FORMATION OF PERIODIC LAYERED STRUCTURE IN TiCu/Zn INTERFACE REACTION[J]. 金属学报, 2014, 50(8): 930-936.
[13] YAN Yongde, YANG Xiaonan, ZHANG Milin, WANG Li, XUE Yun, ZHANG Zhijian. STUDY ON PREPARATION OF Al-Li-Gd ALLOYS BY ELECTROCHEMICAL CODEPOSITION FROM CHLORIDE MELTS[J]. 金属学报, 2014, 50(8): 989-994.
[14] MA Ping, WU Erdong, LI Wuhui, SUN Kai, CHEN Dongfeng. MICROSTRUCTURES AND HYDROGEN STORAGE PROPERTIES OF Ti0.7Zr0.3(Cr1-xVx)2 ALLOYS[J]. 金属学报, 2014, 50(4): 454-462.
[15] GONG Wenbiao, LI Renwei, LI Yupeng,SUN Daqian, WANG Wenquan. STABILIZATION AND CORROSION RESISTANCE UNDER HIGH-TEMPERATURE OF NANOSTRUCTURED CeO2/ZrO2-Y2O3 THERMAL BARRIER COATING[J]. 金属学报, 2013, 49(5): 593-598.
No Suggested Reading articles found!