BRITTLE-TO-DUCTILE TRANSITION TEMPERATURE AND ITS STRAIN RAf E SENSITIVITY IN Ti-47Al-2Mn-2Nb-0.8TiB_2
WANG Yu; LIN Dongliang;T. L. LIN; LIU Junliang; C. C. LAW (The Public Laboratory of State Education Commission for High Temperature Materials and High Temperature Tests; Department of Materials Science;Shanghai Jiaotong University; Shanghai 200030)(Materials & Mechanics Engineering; United Technologies Coporation-Pratt & Whitney; East Hartford;CT 06108; USA)
Cite this article: 

WANG Yu; LIN Dongliang;T. L. LIN; LIU Junliang; C. C. LAW (The Public Laboratory of State Education Commission for High Temperature Materials and High Temperature Tests; Department of Materials Science;Shanghai Jiaotong University; Shanghai 200030)(Materials & Mechanics Engineering; United Technologies Coporation-Pratt & Whitney; East Hartford;CT 06108; USA). BRITTLE-TO-DUCTILE TRANSITION TEMPERATURE AND ITS STRAIN RAf E SENSITIVITY IN Ti-47Al-2Mn-2Nb-0.8TiB_2. Acta Metall Sin, 1998, 34(3): 255-262.

Download:  PDF(3010KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The effect of strain rate on the tensile yield strength and elongation of titanium aluminide has been studied. The alloy has a composition of Ti-47Al-2Mn-2Nb-0.8TiB2 (atomic fraction, %; volume fraction, %, only for TiB2) and near lamellar dricrostructure. It manifests brittle-to-ductile transition (BDT) at elevated temperature and its brittle-to-ductile transition temperature (TBDT) is positively sensitive to the strain rate. The addition of boron lowers the TBDT considerably, and the corresponding activation energy of BDT decreases to 256 kJ/mol, which is less than that of the alloy without boron (TiB2), but approximates the self-diffusion activation energy of atoms in the TiAl alloy. From additional fractography analysis and theoretical estimation, it is suggested that the BDT course of 7 titanium aluminide with the addition of boron (TiB2) is controlled by dislocation climbing.
Key words:  titanium aluminide      intermetullics      BDT      strain rate     
Received:  18 March 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I3/255

1 Kim Y-W. JOM, 1994; 46: 30
2 Huang S C, Hall E L. Metall Trans,1991; 22A: 47
3 Kumpfert J, Kim Y W, Dimiduk D M. Mater Sci Eny, 1995; A192/193: 465
4 王瑜, 林栋梁, 刘俊亮, Law C C. 金属学报, 1997; 33: 1021(Wang Yu, Lin dongliang, Liu Junliang, Law C C. Acta Metall Sin, 1997; 33: 1021)
5 Westwood A R C. Metall Trans, 1988; 19: 749
6 Zener C, Hollomon J. J Appl Phys, 1944; 15: 22
7 Kroll S, Mehrer H, Stolwijk N, Herzig C, Rosenkraus R, Frommeyer G. Z Mettallk, 1992; 83: 591
8 Sprengel W, Oikawa N, Nakajima H. Intermetallics, 1996; 4: 185
9 Nabarro F R N. Philos Mag 1967; 16: 231
10 Schafrik R E. Metall Trans, 1977; 8A: 1003
11 Kad B K, Fraser H L. Philos Mag, 1994; 69: 689
12 Guillard S, Rack H J. Mater Sci Eng, 1994; A183: 181
13 Godfrey A B, Loretto M H. Intermetottics, 1996; 4: 47
14 Kim Y W. In: Kim Y W, Wagner R, Yamaguchi M eds., Gamma Titanium Aboinidea, Warrendale,Pennsylvania: TMS, 1995: 637
15 Pu Z, Wu K-H. Scr Maten 1996; 34: 169M
[1] CHANG Litao. Corrosion and Stress Corrosion Crack Initiation in the Machined Surfaces of Austenitic Stainless Steels in Pressurized Water Reactor Primary Water: Research Progress and Perspective[J]. 金属学报, 2023, 59(2): 191-204.
[2] WANG Kai, JIN Xi, JIAO Zhiming, QIAO Junwei. Mechanical Behaviors and Deformation Constitutive Equations of CrFeNi Medium-Entropy Alloys Under Tensile Conditions from 77 K to 1073 K[J]. 金属学报, 2023, 59(2): 277-288.
[3] WANG Nan, CHEN Yongnan, ZHAO Qinyang, WU Gang, ZHANG Zhen, LUO Jinheng. Effect of Strain Rate on the Strain Partitioning Behavior of Ferrite/Bainite in X80 Pipeline Steel[J]. 金属学报, 2023, 59(10): 1299-1310.
[4] CHEN Yang, MAO Pingli, LIU Zheng, WANG Zhi, CAO Gengsheng. Detwinning Behaviors and Dynamic Mechanical Properties of Precompressed AZ31 Magnesium Alloy Subjected to High Strain Rates Impact[J]. 金属学报, 2022, 58(5): 660-672.
[5] Xiangru GUO, Chaoyang SUN, Chunhui WANG, Lingyun QIAN, Fengxian LIU. Investigation of Strain Rate Effect by Three-Dimensional Discrete Dislocation Dynamics for fcc Single Crystal During Compression Process[J]. 金属学报, 2018, 54(9): 1322-1332.
[6] Xudong LI, Pingli MAO, Yanyu LIU, Zheng LIU, Zhi WANG, Feng WANG. Anisotropy and Deformation Mechanisms ofAs-Extruded Mg-3Zn-1Y Magnesium AlloyUnder High Strain Rates[J]. 金属学报, 2018, 54(4): 557-565.
[7] Xifeng LI, Nannan CHEN, Jiaojiao LI, Xueting HE, Hongbing LIU, Xingwei ZHENG, Jun CHEN. Effect of Temperature and Strain Rate on Deformation Behavior of Invar 36 Alloy[J]. 金属学报, 2017, 53(8): 968-974.
[8] Xu YANG, Bo LIAO, Jian LIU, Wei YAN, Yiyin SHAN, Furen XIAO, Ke YANG. Embrittlement Phenomenon of China Low Activation Martensitic Steel in Liquid Pb-Bi[J]. 金属学报, 2017, 53(5): 513-523.
[9] Yun CAI,Chaoyang SUN,Li WAN,Daijun YANG,Qingjun ZHOU,Zexing SU. STUDY ON THE DYNAMIC RECRYSTALLIZATION SOFTENING BEHAVIOR OF AZ80 MAGNESIUM ALLOY[J]. 金属学报, 2016, 52(9): 1123-1132.
[10] SUN Chaoyang, HUANG Jie, GUO Ning, YANG Jing. A PHYSICAL CONSTITUTIVE MODEL FOR Fe-22Mn-0.6C TWIP STEEL BASED ON DISLOCATION DENSITY[J]. 金属学报, 2014, 50(9): 1115-1122.
[11] LIU Dingming, ZHANG Bo, WANG Jie, WANG Aimin, WANG Yandong, ZHANG Haifeng, HU Zhuangqi. INFLUENCE OF TEMPERATURE ON QUASI-STATIC MECHANICAL PROPERTIES OF Zr-45Ti-5Al-3V ALLOY[J]. 金属学报, 2014, 50(12): 1498-1504.
[12] LIU Yu, LI Yan, LI Qiang. EFFECT OF CATHODIC POLARIZATION ON HYDROGEN EMBRITTLEMENT SUSCEPTIBILITY OF X80 PIPELINE STEEL IN SIMULATED DEEP SEA ENVIRONMENT[J]. 金属学报, 2013, 49(9): 1089-1097.
[13] DONG Danyang, LIU Yang, WANG Lei, SU Liangjin. EFFECT OF STRAIN RATE ON DYNAMIC DEFORMATION BEHAVIOR OF DP780 STEEL[J]. 金属学报, 2013, 49(2): 159-166.
[14] DONG Danyang, LIU Yang, WANG Lei, YANG Yuling, LI Jinfeng, JIN Mengmeng. EFFECT OF STRAIN RATE ON DYNAMIC DEFORMATION BEHAVIOR OF LASER WELDED DP780 STEEL JOINTS[J]. 金属学报, 2013, 49(12): 1493-1500.
[15] ZHANG Bo, FU Huameng, ZHU Zhengwang, ZHANG Haifeng,DONG Chuang,HU Zhuangqi. EFFECT OF W FIBER DIAMETER ON THE COMPRESSIVE MECHANICAL PROPERTIES OF THE Zr-BASED METALLIC GLASS COMPOSITES[J]. 金属学报, 2013, 49(10): 1191-1200.
No Suggested Reading articles found!