STUDY ON NONSTOICHIOMETRIC Mm-Ni SYSTEM HYDROGEN STORAGE ALLOYS |
CHEN Weixiang;TANG Zhiguan;GUO Hetong;CHEN Changpin (Department of Materials Science and Engineering; Zhejiang University; Hangzhou 310027)(Department of Applied Chemistry; Tianjin University; Tianjin 300072) |
|
Cite this article:
CHEN Weixiang;TANG Zhiguan;GUO Hetong;CHEN Changpin (Department of Materials Science and Engineering; Zhejiang University; Hangzhou 310027)(Department of Applied Chemistry; Tianjin University; Tianjin 300072). STUDY ON NONSTOICHIOMETRIC Mm-Ni SYSTEM HYDROGEN STORAGE ALLOYS. Acta Metall Sin, 1998, 34(2): 184-188.
|
Abstract The effects of nonstoichiometric ratio x on the structure, thermodynamic properties for the alloys MmBx (Mm=mischmetal, B=Ni0.72Mn0.08Co0.14Al0.06, x=4.2 - 5.5) and the charge-discharge performances of metal hydride electrodes were investigated. With x value decreasing, the unite cell volumes and the enthalpy (-ΔAH) of hydride formation increased. The relationship of plateau pressure and x of the alloys can be expressed as Inpeq= 1. 99 2x - 11. 131. Asx<5.0, the second phase Ce2Ni7 with high electrocatalytic activity segregated in small numbers in the alloys. The electrodes of nonstoichiometric alloys (x<5.0) had more capacity and superior activation than those of MmB5 and MmB5.5. At x=4.8, the nonstoichiometric alloy electrode had the maximum capacity of 274.7 mA.h/g.
|
Received: 18 February 1998
|
1Nogami M, Tadokoro M, Kimoto M, Chikano Y, Ise T, Furukawa N. Dech Kogaku, 1993; 61: 1088 (in Japanese) 2 Nogami M, Tadokoro M, Kimoto M, Chikano Y, Tse T, Furukawa N. Denki Kagaku, 1993; 61: 1094 (in Japanese) 3 Notten P H L, Hokkeling P.J Electrschem Soc; 1991; 138: 1877 4 Tadokoro M, Nogami M, Chikano Y.J Alloy Comp, 1993; 192: 179 5Muray J I, Post M L,Tayler J B.J Less-Common Met,1981;80:211 6Matsuoka M,Terashima M, Iwakura C. Electrochem Acta,1993;38:108 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|