| STUDY OF INITIAL STAGE SINTERING OF NANOCRYSTALLINE α-Al_2O_3 POWDER BY ISOTHERMAL METHOD |
| LI Jiguang;SUN Xudong;WANG Yarong;DONG Wenxin;RU Hongqiang;HAO Shiming (School of Materials and Metallurgy; Northeastern University; Shenyang 110006) |
|
Cite this article:
LI Jiguang;SUN Xudong;WANG Yarong;DONG Wenxin;RU Hongqiang;HAO Shiming (School of Materials and Metallurgy; Northeastern University; Shenyang 110006). STUDY OF INITIAL STAGE SINTERING OF NANOCRYSTALLINE α-Al_2O_3 POWDER BY ISOTHERMAL METHOD. Acta Metall Sin, 1998, 34(2): 189-194.
|
|
|
Abstract Isothermal sintering method was used to study the initial stage sintering of a soft and a hard agglomerated α-Al2O3 powder with a diameter of 10 nm. For both powders the initial stage sintering was found to be controlled by grain boundary diffusion. Activation energies of grain boundary diffusion of the soft and the hard agglomerated powders were determined to be 354 and 481 kJ/mol respectively and the diffusion coefficient of the soft agglomerated α-Al2O3powder from 900 to 1200 ℃ was estimated.
|
|
Received: 18 February 1998
|
1Johnson D L.J Appl Phys, 1969; 40: 192 2 Young W S, Cutler I B.J Am Ceram Soc, 1970; 53(12): 659 3Johnson D L,Cutler I B.J Am Ceram—Soc, 1963;46(11):545 4Rhodes W H.J Am Ceram Soc,1981;64(1):19 5李继光,孙旭东,茹红强,宋丹,孙祥云,李晓东,郝士明.材料研究学报,待发表 (Li Jiguang, Sun Xudong, Ru Hongqiang, Song Dan, Sun Xiangyun, Li Xiaodong, Hao Shiming. Chn J Mater Res, to be published) 6Roosen A,Hausner H.Adv Ceram Mater,1988;3(2):31 7Johnson D L,Cutler IB.J Am Ceram Soc,1963;46(11):541 8Kingery W D, Berg M, J Appl Phys,1955;26:1205 9Coble R L J.J Am Ceram Soc,1958;41(2):55 |