| APPLICATION OF PATTERN RECOGNITION AND ARTIFICIAL NEURAL NETWORK TO IMPROVE THE MECHANICAL PROPERTIES OF CYLINDER BLOCK CAST OF AUTOMOBILE ENGINE |
| ZHANG Zhaochun; WU Zhu; LI Chonghe; QIN Pei; CHEN Nianyi(Shanghai Institute of Metallurgy; The Chinese Academy of Sciences; Shanghai 200050)Correspondent: WU Zhu; Tel: (021)62511070-8932; Fax: (021)62513510 |
|
Cite this article:
ZHANG Zhaochun; WU Zhu; LI Chonghe; QIN Pei; CHEN Nianyi(Shanghai Institute of Metallurgy; The Chinese Academy of Sciences; Shanghai 200050)Correspondent: WU Zhu; Tel: (021)62511070-8932; Fax: (021)62513510. APPLICATION OF PATTERN RECOGNITION AND ARTIFICIAL NEURAL NETWORK TO IMPROVE THE MECHANICAL PROPERTIES OF CYLINDER BLOCK CAST OF AUTOMOBILE ENGINE. Acta Metall Sin, 1998, 34(10): 1068-1072.
|
|
|
Abstract By means of pattern recoghtion technique the principal factors affecting thetensile strength and hardness of automobile cylinder block cast are discussed, and their optimizedrange determined also. Aritificial neural network, trained by known data, has been used topredict the values of both tensile strength and hardness. The predicted results agree well withthe experimental ones. It has been demonstrated that the mentioned optidsation techniqueprovides a technical approach to disprove the tensile strength and hardness of cylinder block castof automobile engine.
|
|
Received: 18 October 1998
|
1 陈念贻.模式识别优化技术及其应用.北京:中国石化出版社,1997:16(Chen N Y. Technology of Pattern Recognition Optimization and Its Application.Beijing: ChinaPetrocbendcal Industry Press, 1997: 16) 2 Geledi P, Kowalski B R. Anal Chim Acta,1986; 185: 1 3 Beebe K, Kowalski B R. Anal Chem,1987; 59:1007 4 Lippman R P. IEBE Trans Acoust,Speech,Signal Process, 1987; 3: 4 5 Hopheld J J. Proc Natl Acad Sci USA, 1982; 79: 2554Hopfield J J. Proc Natl Acad Sci USA, 1984; 81: 3088 6 王伟,人工神经网络原理──入门与应用北京:北京航空航天大学出版社,1995:62(Wang W. Principle of Neural Network: Elemtary Coarse and Application.Beijing: Beijing Aeronauticsand Asronautics University Press, 1995: 68) 7 中国机械工程学会铸造专业学会编.铸造手册(第一卷,铸铁).北京:机械工业出版社,1997:204,161(Casting Committee of Chinese Mechanical Engineering Society Handbook of Casting. Vol. I, Cast Iron,Beijing: Mechanical Industry Press, 1997: 204, 161)Q |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|