| TEM OBSERVATION OF MICROSTRUCTURES AND FINE STRUCTURES DURING BAINITIC NUCLEATION IN THE STEEL 8Mn8SiMo |
| WU Xiaolei;CHEN Guangnan (Institute of Mechanics; Chinese Academy of Sciences; Beijing 100080); MA Chaoli;KANG Mokuang (Northwestern Polytechntical University; Xi'an 710072) |
|
Cite this article:
WU Xiaolei;CHEN Guangnan (Institute of Mechanics; Chinese Academy of Sciences; Beijing 100080); MA Chaoli;KANG Mokuang (Northwestern Polytechntical University; Xi'an 710072). TEM OBSERVATION OF MICROSTRUCTURES AND FINE STRUCTURES DURING BAINITIC NUCLEATION IN THE STEEL 8Mn8SiMo. Acta Metall Sin, 1997, 33(7): 697-701.
|
|
|
Abstract The microstructure and substructure of the bainitic-ferrite at the most early stage of growth in an Fe-0.79C-8.3Mn-0.87St-0.50Mo steel are studied by TEM. It is observed that the bainite nuclei exhibit a thin plate morphology. And, the bainite formation has the character of catalysis nucleation by sub-units. Moreover, the existence of (lll)f defect plane is firstly observed, and its formation is considered to be the result of the plastic accommodation effect occurred in parent austenite during bainitic nucleation and growth. Defect planes, in fact, to be the glide plane of austenite matrix, consist of part of the bainitic-ferrite/austenite interface. Thus, the formation of bainitic-ferrite is of shear nature.
|
|
Received: 18 July 1997
|
1Aaronson HI, Wells C. Trans AIME, 1956; 206: 1216 2Spanos G, Fang H S, Aaronson HI. Metall Trans, 1990; 21A: 1381 3Hehemann R F. Phase Transbrmation. Metals Park, Ohio: ASM, 1970: 397 4Bhadeshia H K D H, Christian J W. Metall Trans, 1990; 21A: 767 5 Wu X L, Zhang X Y, Kang M K. Mater Trans JIM, 1994; 30: 782 6 Bhadeshia H K D H Bainite in Steels.London:The Institute of Materials,1992:135 7俞德刚,朱钰如,陈大军,唐晓宏,张惠娟.金属学报,1994;30:A385 8孟祥康,康沫狂.金属学报,1993;29:A359 9冯华,康沫狂,李春信.材料科学进展,1988;2(3):32 10Olson G B, Cohen M.Metall Trans,1976; 7A: 1879 11康沫狂,杨延清,张喜燕,孙加林,贾虎生,武晓雷金属学报, 1996; 32: A897 12Sandvik B P J, Wayman C M. Metall Trans, 1983; 14A: 2455 13黄孝瑛.透射电子显微学.上海:上海科学技术出版社,1986:282 |