WU Ximao;Al Suhua;ZHANG Yun;WANG Zhonmang;HAN Xinglin (State Key Laboratory for Fatigue and Fracture of Materials; Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015) (Shenyang Polytechnic University. Shenyang 110023). THE LOW CYCLE FATIGUE BEHAVIOUR FOR 8090 Al-Li ALLOYS. Acta Metall Sin, 1997, 33(7): 702-708.
|
|
|
Abstract Low cycle fatigue property, cyclic hardening and softening of 8090 Al-Li alloys at various aging conditions were studied. The results showed that cyclic response stress in the same aging condition increased with increasing strain amplitude, and aging condition had a little influence on cyclic deformation at low strain amplitude but the influence increased with raising strain amplitude. The characteristics of low cyclic fatigue and cyclic hardening and softening of the alloy were closely related to dislocation morphology, size of precipitate, PFZs along grain boundaries and fracture appearance.
|
|
Received: 18 July 1997
|
1宫木美光,日野光雄金属, 1984; 54(1): 11 2Starke E A Jr, Sanders T H Jr, PalmerlG J. Metall, 1981; 33(8): 24 3Noble B, Hams S J, Dnsdale K J Mater Set, 1982; 17: 461 4Sanders T H Jr, Starke E A]r Acla Melall- 1982; 30: 927 5Quested P N,McLean M,Winstone M R.In:Reichman S,Duhl D N eds,Superalloys 1988,Warrendale, PA: The Metallurgical Society, 1988: 377 6Xu Y B,Wang L,Zhang Y,Wang Z G,Hu Z Q.Metall Trans,1991;22A:723 7Ai Suhua, Wang Zhongguang, Zhang Yun. Trans Non ferrous Melals Soc Chin, 1995; 5(1): 80 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|