SELF GRAIN REFINEMENT OF METALS
BIAN Xiufang; ZHOU Xinguo; LIU Guangrong; LIU Xianfa; MA Jiaji (ShandongUniversity ofTechnology; Ji'nan; 250061)
Cite this article: 

BIAN Xiufang; ZHOU Xinguo; LIU Guangrong; LIU Xianfa; MA Jiaji (ShandongUniversity ofTechnology; Ji'nan; 250061). SELF GRAIN REFINEMENT OF METALS. Acta Metall Sin, 1997, 33(6): 602-608.

Download:  PDF(2721KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A new technology of grain refinement of metals, self grain refinement, obtained by the utilization of the nucleation potential inherent in commercially pure Al, Cu andSb has been described. The effects of the cooling rate, adding amount and holding time inmolten metal for the rapidly solidified sheet of these metals on self grain refinement have beenexamined. The effectiveness of the self grain refinement of aluminium is equal to that of amaster Al-Ti-B added in the aluminium. Cu and Sb also have the effectiveness of the selfgrain refinement. The mechanism of the self grain refinement of metals has been studied onthe heredity theory of metals.
Key words:  self grain refinement      aluminium      copper      stibium     
Received:  18 June 1997     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1997/V33/I6/602

1Mitra P K,Bhattacharya I N.Trans India Inst Met,1986;39(2):150
2著,王永海,张发明,高革译.变形铝合金的细
化处理北京:冶金工业出版社,1988:201
3Flemings M C.Solidification processing,New York:Mc Graw Hill,1974:155
4胡汉起.金属凝固.北京:冶金工业出版社,1985:294
5Hadlet D. Solidification processing,London: The Institute of Metals, 1987: 141
6Spittle J A, Sadlis. Cast Metals, 1995; 7: 247
7Mondolfa L F. Solidification processing, London: The Institute ofMetal, 1987: 133
8 BanerjiA,Reif w.J Mater Sci,1994;29:1958
9安阁英.铸件形成理论.北京:机械工业出版社,1990:147
10铝及铝合金加工制品低倍组织检验方法,GB3247—82
11 Matyia H,Giessen B C,Grant N J.J Inst Met,1968;96:30
12Pearson J,Birch M E J, Haldet D. Solidification Technology in the Foundry and Casthouse, London:Mid—Count Press, 1980: 70
13Ponies P S, de Galiza J A, Robert M H, Cupini N L. Solidification Technology in the Foundry andCasthouse, London: Mid-County Press, 1980: 74
14王广厚.物理学进展,1994;14:121
15蔡英文,范新会,李建国,傅恒志.西北工业大学学报,1996;14:323
16刘相法,边秀房,李辉,马家骥.金属学报,1996;32:149
17 1966:562
18 1940; 10: 942
[1] CHEN Kaixuan, LI Zongxuan, WANG Zidong, Demange Gilles, CHEN Xiaohua, ZHANG Jiawei, WU Xuehua, Zapolsky Helena. Morphological Evolution of Fe-Rich Precipitates in a Cu-2.0Fe Alloy During Isothermal Treatment[J]. 金属学报, 2023, 59(12): 1665-1674.
[2] ZHAO Naiqin, GUO Siyuan, ZHANG Xiang, HE Chunnian, SHI Chunsheng. Progress on Graphene/Copper Composites Focusing on Reinforcement Configuration Design: A Review[J]. 金属学报, 2021, 57(9): 1087-1106.
[3] PENG Wuqingliang, LI Qiang, CHANG Yongqin, WANG Wanjing, CHEN Zhen, XIE Chunyi, WANG Jichao, GENG Xiang, HUANG Lingming, ZHOU Haishan, LUO Guangnan. A Review on the Development of the Heat Sink of the Fusion Reactor Divertor[J]. 金属学报, 2021, 57(7): 831-844.
[4] HUANG Songpeng, PENG Can, CAO Gongwang, WANG Zhenyao. Corrosion Behavior of Copper-Nickel Alloys Protected by BTA in Simulated Urban Atmosphere[J]. 金属学报, 2021, 57(3): 317-326.
[5] CHEN Junzhou, LV Liangxing, ZHEN Liang, DAI Shenglong. Precipitation Strengthening Model of AA 7055 Aluminium Alloy[J]. 金属学报, 2021, 57(3): 353-362.
[6] Jianqiang REN, Shuhua LIANG, Yihui JIANG, Xiang DU. Research on the Microstructure and Properties of In Situ (TiB2-TiB)/Cu Composites[J]. 金属学报, 2019, 55(1): 126-132.
[7] Ran TAO, Yutao ZHAO, Gang CHEN, Xizhou KAI. Microstructure and Properties of In-Situ ZrB2 np/AA6111 Composites Synthesized Under an Electromagnetic Field[J]. 金属学报, 2019, 55(1): 160-170.
[8] Pengyue ZHAO, Yongbo GUO, Qingshun BAI, Feihu ZHANG. Research of Surface Defects of Polycrystalline Copper Nanoindentation Based on Microstructures[J]. 金属学报, 2018, 54(7): 1051-1058.
[9] Tingting ZHAO, Zhixin KANG, Xiayu MA. Fabricating Superhydrophobic Copper Meshes by One-Step Electrodeposition Method and Its Anti-Corrosion and Oil-Water Separation Abilities[J]. 金属学报, 2018, 54(1): 109-117.
[10] Tingbiao GUO, Qi LI, Chen WANG, Feng ZHANG, Zhi JIA. Deformation Characteristics and Mechanical Properties of Single Crystal Copper During Equal Channel Angular Pressing by Route A[J]. 金属学报, 2017, 53(8): 991-1000.
[11] Fenjun LIU, Li FU, Haiyan CHEN. Microstructures and Mechanical Properties of Thin Plate Aluminium Alloy Joint Prepared by High Rotational Speed Friction Stir Welding[J]. 金属学报, 2017, 53(12): 1651-1658.
[12] Wei FU,Xiaoguo SONG,Long LONG,Jianhang CHAI,Jicai FENG,Guodong WANG. INTERFACIAL MICROSTRUCTURE AND MECHANI-CAL PROPERTIES OF INDIRECT BRAZED GRAPHITE/COPPER JOINT[J]. 金属学报, 2016, 52(6): 734-740.
[13] Wei GU,Jingyuan LI,Yide WANG. EFFECT OF GRAIN SIZE AND TAYLOR FACTOR ON THE TRANSVERSE MECHANICAL PROPERTIES OF 7050 ALUMINIUM ALLOY EXTRUSION PROFILE AFTER OVER-AGING[J]. 金属学报, 2016, 52(1): 51-59.
[14] Zhisheng WANG, Xiang CHEN, Yanxiang LI, Huawei ZHANG, Yuan LIU. EFFECTS OF B ON HIGH TEMPERATURE MECHA-NICAL PROPERTIES AND THERMAL FATIGUE BEHAVIOR OF COPPER DIE-CASTING DIE STEEL[J]. 金属学报, 2015, 51(5): 519-526.
[15] Chao YANG,Jijie WANG,Zongyi MA,Dingrui NI,Mingjie FU,Xiaohua LI,Yuansong ZENG. FRICTION STIR WELDING AND LOW-TEMPERATURE SUPERPLASTICITY OF 7B04 Al SHEET[J]. 金属学报, 2015, 51(12): 1449-1456.
No Suggested Reading articles found!