TEXTURE DISTRIBUTION AND DEVELOPMENT THROUGH THE THICKNESS AFTER CROSS SHEAR ROLLING OF GRAIN ORIENTED SILICON STEEL
LIU Gang (Northeastern University; Shenyang 110006; Liaoning University);Shenyang 110036); WANG Fu; QI Kemin;;LIU Guilan; LIANG Zhide (Northeastern University; Shenyang 110006)(Manuscript received 1996-03-20; in revised form 1996-07-10)
Cite this article: 

LIU Gang (Northeastern University; Shenyang 110006; Liaoning University);Shenyang 110036); WANG Fu; QI Kemin;;LIU Guilan; LIANG Zhide (Northeastern University; Shenyang 110006)(Manuscript received 1996-03-20; in revised form 1996-07-10). TEXTURE DISTRIBUTION AND DEVELOPMENT THROUGH THE THICKNESS AFTER CROSS SHEAR ROLLING OF GRAIN ORIENTED SILICON STEEL. Acta Metall Sin, 1997, 33(4): 364-369.

Download:  PDF(553KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Commercial grain oriented silicon steel was cold rolled from 0. 746 mm to 0.34 mm, by cross shear rolling with a roll mismatch speed ratio 1.17, after first cold rolling and intermediate annealing as normal. The subsequent annealing was just as that in industry. The texture distribution and development through the thickness were researched by ODF and reverse pole figure quantitative analyses, and the magnetic properties were measured. The results indicate that the deformation texture is similar to that obtained by traditional one,favorable deformation texture can also be found near the both outer layers of sheet, but they deviate obviously to the fast speed roll. Therefore, the deformation texture shows an asymmetry distribution through the thickness. After decarbon annealing, η-fibre increases,texture with a symmetry distribution reappears through the thickness: sharp Goss texture forms after the secondary recrystallization annealing, and the magnetic properties measured are not lower than that rolled by traditional one.
Key words:  cross shear rolling      silicon steel      texture     
Received:  18 April 1997     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1997/V33/I4/364

1Goss N P.Trans Am Soc Met,1935;23:511
2米泉.钢铁,1980;15(6):1
3刘刚,王彤,王福,齐克敏,梁志德,栗守维,叶久美。电工钢,1995;4:22
4Liu G,Wang F,Qi K M,Liang Z D.Proc 11th Inte Conf on Textures of Materials,Xi’an,China1996:315
5Liang Z,Xu J,Wang F.Proc 6th Int Conf on Textures of Materials,Tokyo:ISIJ,1981:1259
6梁志德,徐家桢,王福。织构材料的三维取向分析术-ODF分析。沈阳:东北工学院出版社,1986;115:151
7罗阳。金属学报,1977;13(1,2):93
8罗阳,吕其春。金属学报,1979;15:235
9Mishra S,Darmann C,Lucke K.Acta Metall,1984; 32:2185
10刘燕声,梁志德.科学通报,1989;34:471
11刘燕声,赵骧,梁志德。金属学报,1990;25:B198
12朱泉等。板材异步轧制理论与实际。沈阳:东北工学院出版社,1984:48
13Bottcher A,Hastenrath M,Lucke K.Textures Microstruct,1991;(14-18):799
[1] CHANG Songtao, ZHANG Fang, SHA Yuhui, ZUO Liang. Recrystallization Texture Competition Mediated by Segregation Element in Body-Centered Cubic Metals[J]. 金属学报, 2023, 59(8): 1065-1074.
[2] LOU Feng, LIU Ke, LIU Jinxue, DONG Hanwu, LI Shubo, DU Wenbo. Microstructures and Formability of the As-Rolled Mg- xZn-0.5Er Alloy Sheets at Room Temperature[J]. 金属学报, 2023, 59(11): 1439-1447.
[3] JIANG Weining, WU Xiaolong, YANG Ping, GU Xinfu, XIE Qingge. Formation of Dynamic Recrystallization Zone and Characteristics of Shear Texture in Surface Layer of Hot-Rolled Silicon Steel[J]. 金属学报, 2022, 58(12): 1545-1556.
[4] YANG Ping, WANG Jinhua, MA Dandan, PANG Shufang, CUI Feng'e. Influences of Composition on the Transformation-Controlled {100} Textures in High Silicon Electrical Steels Prepared by Mn-Removal Vacuum Annealing[J]. 金属学报, 2022, 58(10): 1261-1270.
[5] DING Ning, WANG Yunfeng, LIU Ke, ZHU Xunming, LI Shubo, DU Wenbo. Microstructure, Texture, and Mechanical Properties of Mg-8Gd-1Er-0.5Zr Alloy by Multi-Directional Forging at High Strain Rate[J]. 金属学报, 2021, 57(8): 1000-1008.
[6] YAN Mengqi, CHEN Liquan, YANG Ping, HUANG Lijun, TONG Jianbo, LI Huanfeng, GUO Pengda. Effect of Hot Deformation Parameters on the Evolution of Microstructure and Texture of β Phase in TC18 Titanium Alloy[J]. 金属学报, 2021, 57(7): 880-890.
[7] ZUO Liang, LI Zongbin, YAN Haile, YANG Bo, ZHAO Xiang. Texturation and Functional Behaviors of Polycrystalline Ni-Mn-X Phase Transformation Alloys[J]. 金属学报, 2021, 57(11): 1396-1415.
[8] XU Zhanyi, SHA Yuhui, ZHANG Fang, ZHANG Huabing, LI Guobao, CHU Shuangjie, ZUO Liang. Orientation Selection Behavior During Secondary Recrystallization in Grain-Oriented Silicon Steel[J]. 金属学报, 2020, 56(8): 1067-1074.
[9] YU Lei,LUO Haiwen. Effect of Partial Recrystallization Annealing on Magnetic Properties and Mechanical Properties of Non-Oriented Silicon Steel[J]. 金属学报, 2020, 56(3): 291-300.
[10] CHENG Chao,CHEN Zhiyong,QIN Xushan,LIU Jianrong,WANG Qingjiang. Microstructure, Texture and Mechanical Property ofTA32 Titanium Alloy Thick Plate[J]. 金属学报, 2020, 56(2): 193-202.
[11] DU Zijie, LI Wenyuan, LIU Jianrong, SUO Hongbo, WANG Qingjiang. Study on the Uniformity of Structure and Mechanical Properties of TC4-DT Alloy Deposited by CMT Process[J]. 金属学报, 2020, 56(12): 1667-1680.
[12] Liping DENG,Kaixuan CUI,Bingshu WANG,Hongliang XIANG,Qiang LI. Microstructure and Texture Evolution of AZ31 Mg Alloy Processed by Multi-Pass Compressing Under Room Temperature[J]. 金属学报, 2019, 55(8): 976-986.
[13] Xin LI,Yuecheng DONG,Zhenhua DAN,Hui CHANG,Zhigang FANG,Yanhua GUO. Corrosion Behavior of Ultrafine Grained Pure Ti Processed by Equal Channel Angular Pressing[J]. 金属学报, 2019, 55(8): 967-975.
[14] Zheng LIU,Jianrong LIU,Zibo ZHAO,Lei WANG,Qingjiang WANG,Rui YANG. Microstructure and Tensile Property of TC4 Alloy Produced via Electron Beam Rapid Manufacturing[J]. 金属学报, 2019, 55(6): 692-700.
[15] Houlong LIU,Mingyu MA,Lingling LIU,Liangliang WEI,Liqing CHEN. Effect of Hot Band Annealing Processes on Texture and Formability of 19Cr2Mo1W Ferritic Stainless Steel[J]. 金属学报, 2019, 55(5): 566-574.
No Suggested Reading articles found!