| DIFFUSION OF NITROGEN ATOMS DURING PREPARING Sm_2Fe_(17)N_y MAGNETS BY GAS-SOLID REACTION METHOD |
| ZHOU Shouzeng; YU Shenjun; ZHANG Maocai; WANG Run (University of Sctence and Technology Beijing; Beijing 100083); LIN Guobiao; YIN Youxiang; LIN Yi (Beijing General Institute of Mining and Metallurgy; Beijing 100054) (Manuscript received 1995-10-30; in revised form 1996-04-06) |
|
Cite this article:
ZHOU Shouzeng; YU Shenjun; ZHANG Maocai; WANG Run (University of Sctence and Technology Beijing; Beijing 100083); LIN Guobiao; YIN Youxiang; LIN Yi (Beijing General Institute of Mining and Metallurgy; Beijing 100054) (Manuscript received 1995-10-30; in revised form 1996-04-06). DIFFUSION OF NITROGEN ATOMS DURING PREPARING Sm_2Fe_(17)N_y MAGNETS BY GAS-SOLID REACTION METHOD. Acta Metall Sin, 1996, 32(8): 877-883.
|
|
|
Abstract The diffusion behaviour of N atoms in Sm2Fe17 alloys has been studied. The relationship between the diffusion temperature, the diffusion time with average coneentration of N in samples and the distribution of N concentration in powder particle have been measured. The frequency factor D0 and activation energy Q for N atoms diffusion in Sm2Fe17 particle have been calculated. Using Fick second diffusion law the distribution of N concentration in Sm1Fe17 particles and the relationship between the distribution of N concentration with diffusion temperature, diffusion time and particle size are calculated. The calculated results are consistent with experimental results. Correspondent: (ZHOU Shouzeng, professor, State Key Laboratory of Advanced Melallic Materials, University of Science and Technology Beijing, Beijing 100083)
|
|
Received: 18 August 1996
|
| 1周寿增,杨俊,张茂才,林毅,尹有祥,林国际,金属学报,1994;30;B722KanekoH,KurinoT,UchidaH.In:Hi-Perm.LaboratoryResearehCentreforAdvancedMineralandMaterialsProcessinged.,Proc7thIntSymponMagneticAnisotropyandCoercivityinRare-EarthTransitionMetalAlloys,July1992,Canberra,Australia,TheUniversityofWesternAustralia,1992;3203UchidaH,KoikeU,KamadaK,KoeningerV,MatsumuraY,UchidaHH,KurinoT,KanekoH.In:Hi-Perm.LaboratoryResearchCentreforAdvaneedMineralandMaterialsProeessinged.,Proc7thIntSymponMagneticAnisotropyandCoercivityinRare-EarthTransitionMetalAlloys,July1992,Canberra,Australia,TheUniversityofWestemAustralia,1992:3314KatterM,WeckerJ,KuhrtC,SchultzL.JMagnMater,1992,117:4195于申军.北京科技大学博士学位论文,1995R |