Abstract H08Mn2SiA welding wire was successfully used to joint pure Cu and low carbon steel. Energy dispersive X-ray analysis shows that there is a Fe containing transitional zone of which the width is about few hundreds micron. No thermal cracks and other defects were observed in seam and the tensile strength of seam reached 200 MPa.
|
Received: 18 June 1996
|
1AmericanSocietyforMetals,包芳涵等译.金属手册,第六卷第九版,北京:机械工业出版社,1994:5782CM著,邸斌,刘中青译.有色金属焊接手册.北京:铁道出版社,1988:3183KearnsWH.Weldinghandbook.Vo1.47thedMiami:AmericanWeldingSociety,1982:5334刘中青,邸斌.异种材料的焊接,北京:科学出版社,1990:2315武春芝,刘俊强,叶文太,焊接学报,1990;(4):2250 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|