Please wait a minute...
Acta Metall Sin  1996, Vol. 32 Issue (3): 303-307    DOI:
Current Issue | Archive | Adv Search |
STRUCTURE AND MAGNETIC CHARACTER OF NANOSTRUCTURED NiAl ALLOY SYNTHESIZED BY INERT-GAS CONDENSATION
QIN Xiaoying; ZHANG Lide; HOU Bihui; LIANG Renyou; JI Xiaoli(Institute of Solid State Physics; Chinese Academy of Sciences; Hefei 230031)( University of Science and Technology; Hefei 230026 )(Structure Research Laboratory; University of Science and Technology; Hefei 230026 )(Manuscript received 1995-03-13; in revised form 1995-09-18)
Cite this article: 

QIN Xiaoying; ZHANG Lide; HOU Bihui; LIANG Renyou; JI Xiaoli(Institute of Solid State Physics; Chinese Academy of Sciences; Hefei 230031)( University of Science and Technology; Hefei 230026 )(Structure Research Laboratory; University of Science and Technology; Hefei 230026 )(Manuscript received 1995-03-13; in revised form 1995-09-18). STRUCTURE AND MAGNETIC CHARACTER OF NANOSTRUCTURED NiAl ALLOY SYNTHESIZED BY INERT-GAS CONDENSATION. Acta Metall Sin, 1996, 32(3): 303-307.

Download:  PDF(361KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The structure of nanostructured NiAl(n-NiAl), synthesized by inert-gas condensation, was investigated by X-ray diffraction and TEM. The results indicated that the crystal structure of n-NiAl is same as that of conventional poly-crystalline NiAl alloy(p-NiAl); and the mean grain size of n-NiAl is 8.6 nm. However, there is severe distortion in the crystal lattice of n- NiAl(the distortion ε = 1 .2%); and the long-range ordering degree of n-NiAl is lower than that of p-NiAl. Annealing experiments showed that the grain growth almost did not occur when annealing temperature was lower than 800 K, indicating that n-NiAl is of high resistance to grain growth. In addition, by using electron-spin resonance and magnetization, the strong magnetism(ferro-or antiferromagnetism) of n-NiAl has been ovserved, and it is different from the conventional p-NiAl with weak one. The enhancement of magnetism of n-NiAl would be related to the severe distortion in the crystal lattice and the damage of long-range ordering degree of n-NiAl. Correspondent: QIN Xiaoying, associate professor, Institute of Solid State Physics, Chinese Academy of Sciences, Hefei 230031
Key words:  nanostructured solid      NiAl alloy      structure      magnetism     
Received:  18 March 1996     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1996/V32/I3/303

1DaroliaR.In:DaroliaR,LewandowskkiJJ,LiuCT,etal.eds,StructuralIntermetallics,Warrendale:TMS,1993:4952程天一.金属学报,1994,30:A3993张世远,路权,薛荣华,都有为,磁性材料基础.北京:科学出版社,1988:2244KarchJ,BirringerR,GleiterH.Nature,1987,330:5565苏,吴希俊,秦晓英,谢斌,纪小丽,物理学报,1993,42:9696BirringerR,HerrU,GleiterH.SupplTransJpnInstMet,1986;27:437何崇智,郗秀荣,孟庆恩,佟玉,吕世琴.X射线衍射实验技术.上海科学技术出版社,1988:2838秦晓英,张立德.材料研究学报,待发表
[1] MA Dexin, ZHAO Yunxing, XU Weitai, WANG Fu. Effect of Gravity on Directionally Solidified Structure of Superalloys[J]. 金属学报, 2023, 59(9): 1279-1290.
[2] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[3] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[4] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[5] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[6] CHEN Liqing, LI Xing, ZHAO Yang, WANG Shuai, FENG Yang. Overview of Research and Development of High-Manganese Damping Steel with Integrated Structure and Function[J]. 金属学报, 2023, 59(8): 1015-1026.
[7] LIU Xingjun, WEI Zhenbang, LU Yong, HAN Jiajia, SHI Rongpei, WANG Cuiping. Progress on the Diffusion Kinetics of Novel Co-based and Nb-Si-based Superalloys[J]. 金属学报, 2023, 59(8): 969-985.
[8] LI Jingren, XIE Dongsheng, ZHANG Dongdong, XIE Hongbo, PAN Hucheng, REN Yuping, QIN Gaowu. Microstructure Evolution Mechanism of New Low-Alloyed High-Strength Mg-0.2Ce-0.2Ca Alloy During Extrusion[J]. 金属学报, 2023, 59(8): 1087-1096.
[9] YUAN Jianghuai, WANG Zhenyu, MA Guanshui, ZHOU Guangxue, CHENG Xiaoying, WANG Aiying. Effect of Phase-Structure Evolution on Mechanical Properties of Cr2AlC Coating[J]. 金属学报, 2023, 59(7): 961-968.
[10] SUN Rongrong, YAO Meiyi, WANG Haoyu, ZHANG Wenhuai, HU Lijuan, QIU Yunlong, LIN Xiaodong, XIE Yaoping, YANG Jian, DONG Jianxin, CHENG Guoguang. High-Temperature Steam Oxidation Behavior of Fe22Cr5Al3Mo-xY Alloy Under Simulated LOCA Condition[J]. 金属学报, 2023, 59(7): 915-925.
[11] ZHANG Deyin, HAO Xu, JIA Baorui, WU Haoyang, QIN Mingli, QU Xuanhui. Effects of Y2O3 Content on Properties of Fe-Y2O3 Nanocomposite Powders Synthesized by a Combustion-Based Route[J]. 金属学报, 2023, 59(6): 757-766.
[12] LI Qian, LIU Kai, ZHAO Tianliang. Rust Formation Behavior and Mechanism of Q235 Carbon Steel in 5%NaCl Salt Spray Under Elastic Tensile Stress[J]. 金属学报, 2023, 59(6): 829-840.
[13] FENG Aihan, CHEN Qiang, WANG Jian, WANG Hao, QU Shoujiang, CHEN Daolun. Thermal Stability of Microstructures in Low-Density Ti2AlNb-Based Alloy Hot Rolled Plate[J]. 金属学报, 2023, 59(6): 777-786.
[14] GUO Fu, DU Yihui, JI Xiaoliang, WANG Yishu. Recent Progress on Thermo-Mechanical Reliability of Sn-Based Alloys and Composite Solder for Microelectronic Interconnection[J]. 金属学报, 2023, 59(6): 744-756.
[15] WU Dongjiang, LIU Dehua, ZHANG Ziao, ZHANG Yilun, NIU Fangyong, MA Guangyi. Microstructure and Mechanical Properties of 2024 Aluminum Alloy Prepared by Wire Arc Additive Manufacturing[J]. 金属学报, 2023, 59(6): 767-776.
No Suggested Reading articles found!