| SUPERPLASTICITY OF FeNiBSi ALLOY COATING |
| WEN Jiuba; LI Yanxiang; ZHU Yaomin; XI Jukui(Luoyang Institute of Technology.Luoyang 471039) |
|
Cite this article:
WEN Jiuba; LI Yanxiang; ZHU Yaomin; XI Jukui(Luoyang Institute of Technology.Luoyang 471039). SUPERPLASTICITY OF FeNiBSi ALLOY COATING. Acta Metall Sin, 1995, 31(3): 135-139.
|
|
|
Abstract The compressive superplastic tests at constant temperature were carried out on flame sprayed FeNiBSi alloy coating on GCrls steel. The relationship of superplastic deformation between the coating and the substrate was investigated. After deformed superplastically, the internal cavities in the FeNiBSi alloy coating may be disappeared. and the bonding interface between the coating and the substrate may be metallurgically welded.
|
|
Received: 18 March 1995
|
| 1TangS著.宋玉泉,齐安全译.超塑性力学.长沙:湖南大学出版社,19882李延祥.文九巴.黄金亮,祝要民.金属学报,1994;30:B1363文九巴.洛阳工学院硕士学位论文、1992D |