Please wait a minute...
Acta Metall Sin  1995, Vol. 31 Issue (3): 130-134    DOI:
Current Issue | Archive | Adv Search |
EFFECT OF Bi SEGREGATION ON GRAIN BOUNDARY EMBRITTLEMENT OF Cu BICRYSTALS WITH [001] SYMMETRICAL TILT BOUNDARIES
LI Guanghai; ZHANG Lide (Institute of Solid Siate Physics; Chinese Academy of Sciences;Hefei 230031 )
Cite this article: 

LI Guanghai; ZHANG Lide (Institute of Solid Siate Physics; Chinese Academy of Sciences;Hefei 230031 ). EFFECT OF Bi SEGREGATION ON GRAIN BOUNDARY EMBRITTLEMENT OF Cu BICRYSTALS WITH [001] SYMMETRICAL TILT BOUNDARIES. Acta Metall Sin, 1995, 31(3): 130-134.

Download:  PDF(345KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The effect of Bi segregation at grain boundary on the fracture behaviour and grain boundary embrittlement was studied by using orientationcontrolled Cu bicrystals with [001] symmetrical tilt boundary.The results indicate that the fracture behaviour and fracture stress of Cu-Bi bicrystals depend strongly on the misorientation, and the grain boundary embrittlement is not related to the density of coincidence site lattice of the grain boundary but to the unsegregated grain boundary energy. the higher the grain boundary energy- the stronger the grain boundary embrittlement. The dependence could be explained by considering the boundary-dependent segregation of Bi atoms.
Key words:  Cu bicrystal      [001] symmetrical tilt boundary      Bi segregation      fracture stress      grain boundary embrittlement     
Received:  18 March 1995     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1995/V31/I3/130

1FraczkiewiczA,BiscondiM.JPhysique,1985;46:C4-4972RusselJD,WinterAT.ScrMetall.1985;19:5753VitekV,WangGJ.SurfSci,1984;144:1104HondrosED.McleanD.PhilosMag.1974;29:7715LiGH.WuXJ,CaiM.QiuQ,TangQH.ScrMetallMater,1990;24:21296WuXJ,LiGH,CaiM,QiuQ.TangQH.In:WuBed.,C-MRSInterSymposiaProc1990Bejing,ElesevierSciencePublishers,1991;5:7237WhiteCL,CoghlanWA.MetallTrans.1977;8A:14038SuttonAP.BalluffiRW.ActaMetall,1987;35:2177
[1] II. Fatigue Crack Initiation and Early Growth HU Yunming; WANG Zhongang (State Key Laboratory for Fatigue and Fracture of Materials; Institute ofMetal Research; Chinese Academy of Sciences; Shenyang 110015) (Manuscript received 1996-09-12; in revised form 1997-03-07). CYCLIC DEFORMATION BEHAVIOR AND FATIGUE CRACK INITIATION IN COPPER BICRYSTALS[J]. 金属学报, 1997, 33(8): 824-830.
[2] I. Cyclic Deformation Behavior and Slip Morphology HU Yunming; WANG Zhongguang (State Key Laboratory for Fatigue and Fracture of Materials; Institute of Metal Research; Chinese Academy ofSciences; Shenyang 110015) (Manuscript received 1996-09- 12; in revised form 1997-03-07). CYCLIC DEFORMATION BEHAVIOR AND FATIGUE CRACK INIT1ATION IN COPPER BICRYSTALS[J]. 金属学报, 1997, 33(8): 814-823.
No Suggested Reading articles found!