Please wait a minute...
Acta Metall Sin  1995, Vol. 31 Issue (14): 86-90    DOI:
Current Issue | Archive | Adv Search |
BETTERMENT ON INTERFACE OF C_F/Al COMPOSITES
WANG Yuqing; TANG Fengjun; ZHENG Jiuhong(Institute of Metal Research;Chinese Academy of Sciences;Shenyang 110015); ZHOU Benlian(Institute of Metal Research; International Centre for Materials Phisics; Chinese Academy of Sciences;Shenyang 110015)(Manuscript received 94-03-11;in revised form 94-06-01)
Cite this article: 

WANG Yuqing; TANG Fengjun; ZHENG Jiuhong(Institute of Metal Research;Chinese Academy of Sciences;Shenyang 110015); ZHOU Benlian(Institute of Metal Research; International Centre for Materials Phisics; Chinese Academy of Sciences;Shenyang 110015)(Manuscript received 94-03-11;in revised form 94-06-01). BETTERMENT ON INTERFACE OF C_F/Al COMPOSITES. Acta Metall Sin, 1995, 31(14): 86-90.

Download:  PDF(380KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  An approach to better the interface of the CF/Al composites was carried out on the optimization of the technological parameters for coating of the C fibres and in squeeze casting process. The optimized temperatures of preform, Tf, for bare or PCS SiC-coated C fibres and of molten metal, Tm, Al-10Si matrix seem to be matched by 733 K and 1033 K or 753 K and 1053 K respectively. The quality of interface in composites is different from the coating of C fibres. Such coating, either to retard the interfacial reaction or to better the bonding state, may improve the strength of composites, e.g., increase of strength of a composite up to 89% by PCS SiC-coating and also improvement of wettability by K2ZrF6 solution. The strength of composites increases with the increase of the interfacial shear stress. Furthermore,the optimized shear stress of M40/Al composites with high modulus C fibers is higher than that of the CF/Al composites with low modulus fibers, thus the higher tensile strength was obtained.Correspondent: WANG Yuqing,(associate Professor, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110015)
Key words:  C_F/Al composite      interface      technological parameter      coating      strength     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1995/V31/I14/86

1CoorCR,YunDI,HuntJrWH.inFishmanSGed.,CastReinforcedMetalComposites,ASM,1988:1952ZhangGD,ZhangWD.ProceedofICCM//Ⅷ,USA,Hawsaii,1991:19H3张国定.航空学报,1991;12:B5704WangYuping,ZhouBenlian,WangZouming,ShiChangxu,JMaterSciTechnol,1993;97:75 王玉庆,郑久红,周本濂.金属学报,1994;30:B1946 王玉庆,王作明,刘 敏,周本濂,师昌绪.复合材料学报,1992;9:137 RocherJP,QuenissetJM,NaslainR.JMaterSciLetter,1985;4:1527
[1] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[2] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[3] FENG Qiang, LU Song, LI Wendao, ZHANG Xiaorui, LI Longfei, ZOU Min, ZHUANG Xiaoli. Recent Progress in Alloy Design and Creep Mechanism of γ'-Strengthened Co-Based Superalloys[J]. 金属学报, 2023, 59(9): 1125-1143.
[4] LI Fulin, FU Rui, BAI Yunrui, MENG Lingchao, TAN Haibing, ZHONG Yan, TIAN Wei, DU Jinhui, TIAN Zhiling. Effects of Initial Grain Size and Strengthening Phase on Thermal Deformation and Recrystallization Behavior of GH4096 Superalloy[J]. 金属学报, 2023, 59(7): 855-870.
[5] WANG Zongpu, WANG Weiguo, Rohrer Gregory S, CHEN Song, HONG Lihua, LIN Yan, FENG Xiaozheng, REN Shuai, ZHOU Bangxin. {111}/{111} Near Singular Boundaries in an Al-Zn-Mg-Cu Alloy Recrystallized After Rolling at Different Temperatures[J]. 金属学报, 2023, 59(7): 947-960.
[6] YUAN Jianghuai, WANG Zhenyu, MA Guanshui, ZHOU Guangxue, CHENG Xiaoying, WANG Aiying. Effect of Phase-Structure Evolution on Mechanical Properties of Cr2AlC Coating[J]. 金属学报, 2023, 59(7): 961-968.
[7] LIANG Kai, YAO Zhihao, XIE Xishan, YAO Kaijun, DONG Jianxin. Correlation Between Microstructure and Properties of New Heat-Resistant Alloy SP2215[J]. 金属学报, 2023, 59(6): 797-811.
[8] WANG Furong, ZHANG Yongmei, BAI Guoning, GUO Qingwei, ZHAO Yuhong. First Principles Calculation of Al-Doped Mg/Mg2Sn Alloy Interface[J]. 金属学报, 2023, 59(6): 812-820.
[9] LIU Junpeng, CHEN Hao, ZHANG Chi, YANG Zhigang, ZHANG Yong, DAI Lanhong. Progress of Cryogenic Deformation and Strengthening-Toughening Mechanisms of High-Entropy Alloys[J]. 金属学报, 2023, 59(6): 727-743.
[10] FENG Li, WANG Guiping, MA Kai, YANG Weijie, AN Guosheng, LI Wensheng. Microstructure and Properties of AlCo x CrFeNiCu High-Entropy Alloy Coating Synthesized by Cold Spraying Assisted Induction Remelting[J]. 金属学报, 2023, 59(5): 703-712.
[11] HUANG Ding, QIAO Yanxin, YANG Lanlan, WANG Jinlong, CHEN Minghui, ZHU Shenglong, WANG Fuhui. Effect of Shot Peening of Substrate Surface on Cyclic Oxidation Behavior of Sputtered Nanocrystalline Coating[J]. 金属学报, 2023, 59(5): 668-678.
[12] WANG Bin, NIU Mengchao, WANG Wei, JIANG Tao, LUAN Junhua, YANG Ke. Microstructure and Strength-Toughness of a Cu-Contained Maraging Stainless Steel[J]. 金属学报, 2023, 59(5): 636-646.
[13] WANG Jingyang, SUN Luchao, LUO Yixiu, TIAN Zhilin, REN Xiaomin, ZHANG Jie. Rare Earth Silicate Environmental Barrier Coating Material: High-Entropy Design and Resistance to CMAS Corrosion[J]. 金属学报, 2023, 59(4): 523-536.
[14] ZHANG Zhefeng, LI Keqiang, CAI Tuo, LI Peng, ZHANG Zhenjun, LIU Rui, YANG Jinbo, ZHANG Peng. Effects of Stacking Fault Energy on the Deformation Mechanisms and Mechanical Properties of Face-Centered Cubic Metals[J]. 金属学报, 2023, 59(4): 467-477.
[15] WAN Tao, CHENG Zhao, LU Lei. Effect of Component Proportion on Mechanical Behaviors of Laminated Nanotwinned Cu[J]. 金属学报, 2023, 59(4): 567-576.
No Suggested Reading articles found!