Please wait a minute...
Acta Metall Sin  1994, Vol. 30 Issue (3): 139-144    DOI:
Current Issue | Archive | Adv Search |
ENVIRONMENTAL EMBRITTLEMENT IN Fe_3Al BASED ALLOYS
ZHU Jiahong;WAN Xiaojing(Shanghai University of Technology)(Manuscript received 1 April;1993;in revised form 8 July;1993)
Cite this article: 

ZHU Jiahong;WAN Xiaojing(Shanghai University of Technology)(Manuscript received 1 April;1993;in revised form 8 July;1993). ENVIRONMENTAL EMBRITTLEMENT IN Fe_3Al BASED ALLOYS. Acta Metall Sin, 1994, 30(3): 139-144.

Download:  PDF(481KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The effect of various factors which include grain size/grain shape,strain rate and preoxidation,on environmental embrittlement of Fe_3Al based alloys has been investigated.Fe_3Al specimens with refined grain or columnar grain structure exhibit improved ductility and strength in both oxygen and air,however,the alloys still demonstrate severe environmental degradation.The severity of embrittlement is identical in air and gaseous hydrogen.As the strain rate increases,the ductility of Fe_3Al in both air and hydrogen is improved.Preoxidation can partly eliminate the environmental effect in Fe_3(Al,Cr,B) alloy.Surfaee reaction is supposed to be the controlling step in environment induced embrittlement of Fe_3Al based alloys.Correspondent:WAN Xiaojing,professor,Shanghai University of Technology,Shanghai 200072
Key words:  Fe_3Al based alloy      environmental embrittlement      strain rate      preoxidation     
Received:  18 March 1994     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1994/V30/I3/139

1MarcinkowskiMJ,TaylorME,KayerFX.JMaterSci,1975;10:4062LiuCT,McKameyCG,LeeEH.ScrMetall1990;24:12813McKameyCG,LiuCT.ScrMetall1990;24:21194LiuCT,McKameyCG,LeeEH.ScrMetall,1990;24:3855LiuCT,McKameyCG.In:WhangSH,LiuCT,PopeDP,StieglerJO,eds.,HighTemperatureAluminidesandIntermetallics,Warrendale,PA,TMS,1990:1336LiuCT.In:LiuCTetaleds.,OrderedIntermetallics-Physical MetallurgyandMechanicalBehaviour,KluwerPublishers,1992:3217WanXJ,ZhuJH,JingKL.ScrMetall,1992;26:4738LiuCT,Kim Y-w.ScrMetallMater.1992;27:5999MasahashiN,TakasugiT,IzumiO,MetallTrans,1988;19A:35310ZhuJH,WanXJWuY.ScrMetallMater,1993;29:42911MarcusP,OudarJ.In:OrianiRA,HirthJP,SmialowskiM,eds.,HydrogenDegradationofFerrousAlloys,NoyesPublications,1985:3612WeiRP,GaoM.InRef.11:579
[1] CHANG Litao. Corrosion and Stress Corrosion Crack Initiation in the Machined Surfaces of Austenitic Stainless Steels in Pressurized Water Reactor Primary Water: Research Progress and Perspective[J]. 金属学报, 2023, 59(2): 191-204.
[2] WANG Kai, JIN Xi, JIAO Zhiming, QIAO Junwei. Mechanical Behaviors and Deformation Constitutive Equations of CrFeNi Medium-Entropy Alloys Under Tensile Conditions from 77 K to 1073 K[J]. 金属学报, 2023, 59(2): 277-288.
[3] WANG Nan, CHEN Yongnan, ZHAO Qinyang, WU Gang, ZHANG Zhen, LUO Jinheng. Effect of Strain Rate on the Strain Partitioning Behavior of Ferrite/Bainite in X80 Pipeline Steel[J]. 金属学报, 2023, 59(10): 1299-1310.
[4] CHEN Yang, MAO Pingli, LIU Zheng, WANG Zhi, CAO Gengsheng. Detwinning Behaviors and Dynamic Mechanical Properties of Precompressed AZ31 Magnesium Alloy Subjected to High Strain Rates Impact[J]. 金属学报, 2022, 58(5): 660-672.
[5] Xiangru GUO, Chaoyang SUN, Chunhui WANG, Lingyun QIAN, Fengxian LIU. Investigation of Strain Rate Effect by Three-Dimensional Discrete Dislocation Dynamics for fcc Single Crystal During Compression Process[J]. 金属学报, 2018, 54(9): 1322-1332.
[6] Xudong LI, Pingli MAO, Yanyu LIU, Zheng LIU, Zhi WANG, Feng WANG. Anisotropy and Deformation Mechanisms ofAs-Extruded Mg-3Zn-1Y Magnesium AlloyUnder High Strain Rates[J]. 金属学报, 2018, 54(4): 557-565.
[7] Xifeng LI, Nannan CHEN, Jiaojiao LI, Xueting HE, Hongbing LIU, Xingwei ZHENG, Jun CHEN. Effect of Temperature and Strain Rate on Deformation Behavior of Invar 36 Alloy[J]. 金属学报, 2017, 53(8): 968-974.
[8] Xu YANG, Bo LIAO, Jian LIU, Wei YAN, Yiyin SHAN, Furen XIAO, Ke YANG. Embrittlement Phenomenon of China Low Activation Martensitic Steel in Liquid Pb-Bi[J]. 金属学报, 2017, 53(5): 513-523.
[9] Yun CAI,Chaoyang SUN,Li WAN,Daijun YANG,Qingjun ZHOU,Zexing SU. STUDY ON THE DYNAMIC RECRYSTALLIZATION SOFTENING BEHAVIOR OF AZ80 MAGNESIUM ALLOY[J]. 金属学报, 2016, 52(9): 1123-1132.
[10] SUN Chaoyang, HUANG Jie, GUO Ning, YANG Jing. A PHYSICAL CONSTITUTIVE MODEL FOR Fe-22Mn-0.6C TWIP STEEL BASED ON DISLOCATION DENSITY[J]. 金属学报, 2014, 50(9): 1115-1122.
[11] LIU Dingming, ZHANG Bo, WANG Jie, WANG Aimin, WANG Yandong, ZHANG Haifeng, HU Zhuangqi. INFLUENCE OF TEMPERATURE ON QUASI-STATIC MECHANICAL PROPERTIES OF Zr-45Ti-5Al-3V ALLOY[J]. 金属学报, 2014, 50(12): 1498-1504.
[12] LIU Yu, LI Yan, LI Qiang. EFFECT OF CATHODIC POLARIZATION ON HYDROGEN EMBRITTLEMENT SUSCEPTIBILITY OF X80 PIPELINE STEEL IN SIMULATED DEEP SEA ENVIRONMENT[J]. 金属学报, 2013, 49(9): 1089-1097.
[13] DONG Danyang, LIU Yang, WANG Lei, SU Liangjin. EFFECT OF STRAIN RATE ON DYNAMIC DEFORMATION BEHAVIOR OF DP780 STEEL[J]. 金属学报, 2013, 49(2): 159-166.
[14] DONG Danyang, LIU Yang, WANG Lei, YANG Yuling, LI Jinfeng, JIN Mengmeng. EFFECT OF STRAIN RATE ON DYNAMIC DEFORMATION BEHAVIOR OF LASER WELDED DP780 STEEL JOINTS[J]. 金属学报, 2013, 49(12): 1493-1500.
[15] ZHANG Bo, FU Huameng, ZHU Zhengwang, ZHANG Haifeng,DONG Chuang,HU Zhuangqi. EFFECT OF W FIBER DIAMETER ON THE COMPRESSIVE MECHANICAL PROPERTIES OF THE Zr-BASED METALLIC GLASS COMPOSITES[J]. 金属学报, 2013, 49(10): 1191-1200.
No Suggested Reading articles found!