Please wait a minute...
Acta Metall Sin  1994, Vol. 30 Issue (18): 254-258    DOI:
Current Issue | Archive | Adv Search |
PREPARATION OF NANO-PARTICLES OF AMORPHOUS Ni-Ti ALLOY BY GAS EVAPORATION METHOD
YANG Mingchuan; XU Jian; SUN Hiukui; WEI Wenduo; HU Zhuangqi(State Key Laboratory of RSA; Institute of Metal Research; Chinese Academy of Scicnces;Shenyang)
Cite this article: 

YANG Mingchuan; XU Jian; SUN Hiukui; WEI Wenduo; HU Zhuangqi(State Key Laboratory of RSA; Institute of Metal Research; Chinese Academy of Scicnces;Shenyang). PREPARATION OF NANO-PARTICLES OF AMORPHOUS Ni-Ti ALLOY BY GAS EVAPORATION METHOD. Acta Metall Sin, 1994, 30(18): 254-258.

Download:  PDF(373KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Parameters of gas evaporation method to prepare the nano-particles of amorphous Ni-Ti alloy have been investigated. The particles obtained were characterised by TEM, HREM, XRD and EDAX. It seems to form easily the amorphous nano-particles under some lower pressure of the inert gas and higher evaporating temperature within a composition range near Ni40Ti60 eutectic.
Key words:  amorphous alloy      nano-particle      gas evaporation     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1994/V30/I18/254

1WonterghemJVan,MorupS,CharlesSW,WellsS,VilladsenJ.PhysRevLetl,1985;55:4102WeissmullerJ,BirringerR,GleiterH.PhysLett,1990;A145:1303JingJ,KramerA,BirrigerR,GleiterH,GonserV.JNon-CrystSolids,1989;113:1674YatsuyaS,YanagidaA,YamauchiK,MihamaK.JCrystGrowth,1984;70:5365徐坚,孙秀魁,陈文绣,范学书,魏文锋.材料科学进展,1992;6:2096UyedaR.ProgMaterSci,1991;35:2237BuschowKHJ.JApplPhys,1984;56:3048KaitoC,FujitaK,ShijiriM.JApplPhys,1976;47:5161
[1] LIU Shuaishuai, HOU Chaonan, WANG Engang, JIA Peng. Plastic Rheological Behaviors of Zr61Cu25Al12Ti2 and Zr52.5Cu17.9Ni14.6Al10Ti5 Amorphous Alloys in the Supercooled Liquid Region[J]. 金属学报, 2022, 58(6): 807-815.
[2] LI Jinfu, LI Wei. Structure and Glass-Forming Ability of Al-Based Amorphous Alloys[J]. 金属学报, 2022, 58(4): 457-472.
[3] ZHANG Jinyong, ZHAO Congcong, WU Yijin, CHEN Changjiu, CHEN Zheng, SHEN Baolong. Structural Characteristic and Crystallization Behavior of the (Fe0.33Co0.33Ni0.33)84 -x Cr8Mn8B x High-Entropy-Amorphous Alloy Ribbons[J]. 金属学报, 2022, 58(2): 215-224.
[4] HAN Luhui, KE Haibo, ZHANG Pei, SANG Ge, HUANG Huogen. Kinetic Crystallization Behavior of Amorphous U60Fe27.5Al12.5 Alloy[J]. 金属学报, 2022, 58(10): 1316-1324.
[5] HU Xiang, GE Jiacheng, LIU Sinan, FU Shu, WU Zhenduo, FENG Tao, LIU Dong, WANG Xunli, LAN Si. Combustion Mechanism of Fe-Nb-B-Y Amorphous Alloys with an Anomalous Exothermic Phenomenon[J]. 金属学报, 2021, 57(4): 542-552.
[6] LIU Riping, MA Mingzhen, ZHANG Xinyu. New Development of Research on Casting of Bulk Amorphous Alloys[J]. 金属学报, 2021, 57(4): 515-528.
[7] ZHU Min, OUYANG Liuzhang. Kinetics Tuning and Electrochemical Performance of Mg-Based Hydrogen Storage Alloys[J]. 金属学报, 2021, 57(11): 1416-1428.
[8] HUANG Huogen, ZHANG Pengguo, ZHANG Pei, WANG Qinguo. Comparison of Glass Forming Ability Between U-Co and U-Fe Base Systems[J]. 金属学报, 2020, 56(6): 849-854.
[9] GENG Yaoxiang, WANG Yingmin. Local Structure-Property Correlation of Fe-Based Amorphous Alloys: Based on Minor Alloying Research[J]. 金属学报, 2020, 56(11): 1558-1568.
[10] XU Xiuyue, LI Yanhui, ZHANG Wei. Fabrication of Nanoporous PtRuFe by Dealloying Amorphous Fe(Pt, Ru)B Ribbons and Their Methanol Electrocatalytic Properties[J]. 金属学报, 2020, 56(10): 1393-1400.
[11] JIN Chenri, YANG Suyuan, DENG Xueyuan, WANG Yangwei, CHENG Xingwang. Effect of Nano-Crystallization on Dynamic Compressive Property of Zr-Based Amorphous Alloy[J]. 金属学报, 2019, 55(12): 1561-1568.
[12] Hongyang XU,Haibo KE,Huogen HUANG,Pei ZHANG,Pengguo ZHANG,Tianwei LIU. Nanoindentation Creep Behavior of U65Fe30Al5 Amorphous Alloy[J]. 金属学报, 2017, 53(7): 817-823.
[13] Dianguo MA,Yingmin WANG,Kunio YUBUTA,Yanhui LI,Wei ZHANG. Effect of Co Content on the Structure and Magnetic Properties of Melt-Spun Fe55-xCoxPt15B30 Alloys[J]. 金属学报, 2017, 53(5): 609-614.
[14] Huogen HUANG,Hongyang XU,Pengguo ZHANG,Yingmin WANG,Haibo KE,Pei ZHANG,Tianwei LIU. U-Cr Binary Alloys with Anomalous Glass-Forming Ability[J]. 金属学报, 2017, 53(2): 233-238.
[15] Yaoxiang GENG,Kaiming HAN,Yingmin WANG,Jianbing QIANG,Qing WANG,Chuang DONG,Guifeng ZHANG,O TEGUS,Peter HAÜSSLER. COMPOSITION DESIGN OF Fe-B-Si-Ta BULK AMORPHOUS ALLOYS BASED ON CLUSTER+ GLUE ATOM MODEL[J]. 金属学报, 2015, 51(8): 1017-1024.
No Suggested Reading articles found!