| ELECTROCHEMICAL IMPEDANCE OF HOT CORROSION OF SPUTTERED CoCrAlY COATING ON Ni_3Al And Ni_3Al-Fe INTERMETALLICS |
| ZENG Chaoliu; ZHANG Jianqing;WU Weitao; NIU Yan(Corrosion Science Lab Oratory; Institute of Corrosion and Protection of Metals; Chinese Academy of Sciences; Shenyang) |
|
Cite this article:
ZENG Chaoliu; ZHANG Jianqing;WU Weitao; NIU Yan(Corrosion Science Lab Oratory; Institute of Corrosion and Protection of Metals; Chinese Academy of Sciences; Shenyang). ELECTROCHEMICAL IMPEDANCE OF HOT CORROSION OF SPUTTERED CoCrAlY COATING ON Ni_3Al And Ni_3Al-Fe INTERMETALLICS. Acta Metall Sin, 1994, 30(18): 247-253.
|
|
|
Abstract The electrochemical impedance combined with physical analysis techniques was employed to study the effect of sputtered CoCrAlY coating on hot corrosion of Ni3Al and Ni3Al-Fe intermetallics. It is shown that Ni3Al and Ni3Al-Fe suffer severe hot corrosion, and their Nyquist diagrams are composed of a semicircle at high frequency portion and a line at low frequency portion, which means the diffusion-controlled reaction.The Nyquist plots of sputtered CoCrAlY coating are composed of two capacitive loops, which means the pitting corrosion. Equivalent circuits to interprete the features of the impedance are proposed, and the parameters in the equivalent circuits are also calculated.
|
|
|
| 1MansfeldF,KendigM,TsaiS.Corrosion,1982;38:4782武成详,西方笃,水流切,武井厚.日本金属学会志,1992;56:11613LiuCT,DevereuxOF.JElectrochemSoc,1991;138:3864WuYM,RappRA.JElectrochemSoc,1991;138:26835张鉴清,曾潮流,牛焱,吴维.中国腐蚀与防护学报,1993;13:2746曾潮流,张鉴清,牛焱,吴维.腐蚀科学与防护技术,1993;5:2297牛焱,张鉴清,吴维.中国腐蚀与防护学报,1990;10:2218王佳,施存余,宋诗哲.中国腐蚀与防护学报,1989;9:129吴维,曾潮流,张鉴清.金属学报,1992;28:B298h |