| CRITICAL VOID-GROWTH STATE AND RELATED FRACTURE TOUGHNESS IN BHW60 STEEL |
| ZHOU Li;ZHENG Changqing;LU Zhixian;DING Fulian Northwestern Polyechnical University; Xi'an Iron and Steel Research Institute; Shanghai Baoshan Steel WorksDepartment of Engineering Mechanics;Northwestern Poly technical Uni versity; Xi'an 710072. |
|
Cite this article:
ZHOU Li;ZHENG Changqing;LU Zhixian;DING Fulian Northwestern Polyechnical University; Xi'an Iron and Steel Research Institute; Shanghai Baoshan Steel WorksDepartment of Engineering Mechanics;Northwestern Poly technical Uni versity; Xi'an 710072.. CRITICAL VOID-GROWTH STATE AND RELATED FRACTURE TOUGHNESS IN BHW60 STEEL. Acta Metall Sin, 1993, 29(8): 44-48.
|
|
|
Abstract The critical void-grwoth ratio, R_c/ R_o, was measured quantitatively underSEM to the core of fracture surface of smooth and notched tensile specimens for BHW60steel at 20, -60, -100 and -140℃. Correlation between R_c/ R_0 and macroscopic fracturetoughness, V_(GC), as well as the effect of heat treated condition upon them were investigated.Results show that the R_c/ R_0 values are approximately obedient to normal probability dis-tribution at the same temperature, decrease linearly with the decrease of temperature and arerelated to V_(GC) as: V(GC)= Cln(R_c/ R_0), where C=3.5. This expression seems to be in goodagreement with the R-T model of void-grwoth and the coefficient C is insensitive to temper-ature and heat treated condition.
|
|
Received: 18 August 1993
|
1 张以增.金属学报,1983;19:A70 2 郑长卿,Radon J C.西北工业大学学报,1985;3:409 3 Garrison W M.Scr Metall, 1984, 18:583 4 郑长卿,Radon J C.西北工业大学学报,1985;3:21 5 Zheng C Q, Zhou L, Liu J M. In: Yan M G Zhang S H, Zheng Z M eds., Mechanical Behaviour of Materials-V, Vol. Ⅰ, Oxford: pergamon, 1987; 213 6 Zhou L, Zheng C Q. In: Zhang Z M, Li F N eds., Proceedings of the Ⅳ Conference of Asian--Pacific Congress on Strength Evaluation (APCS--91) , Vol. Ⅱ. International Academic publishers. 1991: 1079 7 Rice J R, Tracey D M. J Mech Phys Solids. 1969; 17: 201 |
| No Suggested Reading articles found! |
|
|