Please wait a minute...
Acta Metall Sin  1993, Vol. 29 Issue (5): 92-96    DOI:
Current Issue | Archive | Adv Search |
SYNTHESIS OF TiAl+TiB_2 COMPOSITE AND ITS THERMAL STABILITY
HUANG Baiyun;LEI Changming;CHEN Shiqi Central South University of Technology; ChangshaQU Xuanhui;professor;Powder Metallurgy Research Institute; Central South University of Technology;Changsha 410083
Cite this article: 

HUANG Baiyun;LEI Changming;CHEN Shiqi Central South University of Technology; ChangshaQU Xuanhui;professor;Powder Metallurgy Research Institute; Central South University of Technology;Changsha 410083. SYNTHESIS OF TiAl+TiB_2 COMPOSITE AND ITS THERMAL STABILITY. Acta Metall Sin, 1993, 29(5): 92-96.

Download:  PDF(942KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Synthesis process of a TiAl+TiB_2 composite from Ti, Al and B powders wasstudied by means of differential scanning calorimetry and X-ray diffractometry. TiB_2 parti-cles may form in TiAl matrix at temperatures even below 700℃ owing to the exothermic reac-tion between Ti and Al powders. TiB_2 particles are very thermally stable, and almost no morechanged in their relative amount, morphology and size after the synthesized composite beingremelted. In addition, the existence of TiB_2 particles may be obviously affected on refinementof as-cast TiAl-base alloy microstructure.
Key words:  TiAl alloy      TiB_2      composite      thermal stability     
Received:  18 May 1993     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1993/V29/I5/92

1 Lipsitt H A. Mater Res Soc Symp Proc. 1985; 39: 351
2 曲选辉,黄伯云,吕海波,黄培云.稀有金属材料与工程,1991;20(4) :3
3 Kim Y W, Dimidek D M. J Met, 1991; 43 (8) : 40
4 黄培云.粉末冶金原理.北京:冶金工业出版社,1982:407
5 Kampe S I, Bryant J D, Christodoulou L. Metall Trans, 1991; 22A: 447
6 Westwood A R C. Metall Trans, 1988; 19A: 749
7 Brandes E A. Smithells Metals Reference Book. 6th ed, London: Butterworths, 1983: chap 11. pp 29, 52, 105p
[1] YUAN Jianghuai, WANG Zhenyu, MA Guanshui, ZHOU Guangxue, CHENG Xiaoying, WANG Aiying. Effect of Phase-Structure Evolution on Mechanical Properties of Cr2AlC Coating[J]. 金属学报, 2023, 59(7): 961-968.
[2] FENG Aihan, CHEN Qiang, WANG Jian, WANG Hao, QU Shoujiang, CHEN Daolun. Thermal Stability of Microstructures in Low-Density Ti2AlNb-Based Alloy Hot Rolled Plate[J]. 金属学报, 2023, 59(6): 777-786.
[3] ZHANG Deyin, HAO Xu, JIA Baorui, WU Haoyang, QIN Mingli, QU Xuanhui. Effects of Y2O3 Content on Properties of Fe-Y2O3 Nanocomposite Powders Synthesized by a Combustion-Based Route[J]. 金属学报, 2023, 59(6): 757-766.
[4] MA Zongyi, XIAO Bolv, ZHANG Junfan, ZHU Shize, WANG Dong. Overview of Research and Development for Aluminum Matrix Composites Driven by Aerospace Equipment Demand[J]. 金属学报, 2023, 59(4): 457-466.
[5] MA Guonan, ZHU Shize, WANG Dong, XIAO Bolv, MA Zongyi. Aging Behaviors and Mechanical Properties of SiC/Al-Zn-Mg-Cu Composites[J]. 金属学报, 2023, 59(12): 1655-1664.
[6] JIANG Jiang, HAO Shijie, JIANG Daqiang, GUO Fangmin, REN Yang, CUI Lishan. Quasi-Linear Superelasticity Deformation in an In Situ NiTi-Nb Composite[J]. 金属学报, 2023, 59(11): 1419-1427.
[7] LI Xiaobing, QIAN Kun, SHU Lei, ZHANG Mengshu, ZHANG Jinhu, CHEN Bo, LIU Kui. Effect of W Content on the Phase Transformation Behavior in Ti-42Al-5Mn- xW Alloy[J]. 金属学报, 2023, 59(10): 1401-1410.
[8] SHEN Yingying, ZHANG Guoxing, JIA Qing, WANG Yumin, CUI Yuyou, YANG Rui. Interfacial Reaction and Thermal Stability of the SiCf/TiAl Composites[J]. 金属学报, 2022, 58(9): 1150-1158.
[9] LIU Renci, WANG Peng, CAO Ruxin, NI Mingjie, LIU Dong, CUI Yuyou, YANG Rui. Influence of Thermal Exposure at 700oC on the Microstructure and Morphology in the Surface of β-Solidifying γ-TiAl Alloys[J]. 金属学报, 2022, 58(8): 1003-1012.
[10] CHEN Yuyong, YE Yuan, SUN Jianfei. Present Status for Rolling TiAl Alloy Sheet[J]. 金属学报, 2022, 58(8): 965-978.
[11] GU Ruicheng, ZHANG Jian, ZHANG Mingyang, LIU Yanyan, WANG Shaogang, JIAO Da, LIU Zengqian, ZHANG Zhefeng. Fabrication of Mg-Based Composites Reinforced by SiC Whisker Scaffolds with Three-Dimensional Interpenetrating-Phase Architecture and Their Mechanical Properties[J]. 金属学报, 2022, 58(7): 857-867.
[12] ZHENG Shijian, YAN Zhe, KONG Xiangfei, ZHANG Ruifeng. Interface Modifications on Strength and Plasticity of Nanolayered Metallic Composites[J]. 金属学报, 2022, 58(6): 709-725.
[13] PAN Chengcheng, ZHANG Xiang, YANG Fan, XIA Dahai, HE Chunnian, HU Wenbin. Corrosion and Cavitation Erosion Behavior of GLNN/Cu Composite in Simulated Seawater[J]. 金属学报, 2022, 58(5): 599-609.
[14] WANG Haowei, ZHAO Dechao, WANG Mingliang. A Review of the Corrosion Protection Technology on In SituTiB2/Al Composites[J]. 金属学报, 2022, 58(4): 428-443.
[15] ZHANG Lei, SHI Tao, HUANG Huogen, ZHANG Pei, ZHANG Pengguo, WU Min, FA Tao. Phase Separation and Solidification Sequence of Uranium-Based Amorphous Composites[J]. 金属学报, 2022, 58(2): 225-230.
No Suggested Reading articles found!