| EFFECT OF Mg SEGREGATION AT GRAIN BOUNDARIES ON CORROSION BEHAVIOUR OF Ni_3Al(0.1B) |
| JIANG Bingyao;WANG Xi;SUN Jian;ZOU Shichang Ion Beam Laboratory; Shanghai Institute of Metallurgy; Academia SinicaLIU Xianghuai;professor;Shanghai Institule of Metallurgy.Academia Siniea;Shanghai 20005 |
|
Cite this article:
JIANG Bingyao;WANG Xi;SUN Jian;ZOU Shichang Ion Beam Laboratory; Shanghai Institute of Metallurgy; Academia SinicaLIU Xianghuai;professor;Shanghai Institule of Metallurgy.Academia Siniea;Shanghai 20005. EFFECT OF Mg SEGREGATION AT GRAIN BOUNDARIES ON CORROSION BEHAVIOUR OF Ni_3Al(0.1B). Acta Metall Sin, 1993, 29(5): 87-91.
|
|
|
Abstract Dose of 1×10~(16) Mg~+ ion / cm~2 with 120 keV was implanted into theintermetallic compound Ni_3Al(0.1B). Studies were made of the corrosion behaviour bymulti-sweep cyclic voltammetry and optical microscopy. The corrosion resistance of the spec-imen after implanting by Mg~+ ions may be much improved to 0.5mol/L H_2SO_4 solution.Experimental measurements and computer simulation were carried out on the segregation ofMg atoms at the grain boundaries. Mechanism of beneficial effect of Mg~+ ion implantationon corrosion resistance was approaching.
|
|
Received: 18 May 1993
|
1 Liu Xianghuai. Zheng Zhihong, Huang Wei, Lin Zixin. Wang Xi, Yang Genqing, Zou Shichang, Taniguchi S, Shibata T. Ion Sci Technol, 1991; 191: 121 2 孙超,郭建亭,李辉,谭明晖,赖万慧,王淑荷.见:仲增墉.叶恒强主编,金属间化合物--全国首届高温结构金属间化合物学术讨论会论文集,北京:机械工业出版社,1992:99 3 Liu Xianghuai, Zou Shichang. Taniguchi S. Fang Qinxue, Kalbitzer S, Schroer A, Fischer W, Barth M, Ensinger W, Wolf G K. Nucl Instrum Methods Phys Res, 1991: B59/60: 851 4 Kim Y G. Yoon G W, Stoloff N S. Metall Trans, 1985; A16: 2072 5 Chen S P, Voter A F, Albers R C, Boring A M, Hay P J. J Mater Res, 1990: 5: 955 |
| No Suggested Reading articles found! |
|
|