| FATIGUE CRACK INITIATION ON NON-OVERLAPPED LASER HARDENED 40Cr STEEL |
| LIU Changsheng;CAI Qingkui;XU Hao Northeastern University; Shenyang |
|
Cite this article:
LIU Changsheng;CAI Qingkui;XU Hao Northeastern University; Shenyang. FATIGUE CRACK INITIATION ON NON-OVERLAPPED LASER HARDENED 40Cr STEEL. Acta Metall Sin, 1993, 29(12): 34-38.
|
|
|
Abstract Study was carried out of the effect of overlapping or not on the fatiguemacro-crack initiation on the notch root of 40Cr steel specimens treated by newly developedtechnique of laser local hardening. The resistance to fatigue macro-crack initiation may bemade by grain refining, marstrengthening and residual compressive stress. In the light ofbehaviour of fatigue fracture, the superiority of local laser hardening to improve the fatigueresistance is in the range of low stress amplitude and high cycles. The morphology of the frac-ture surface in the hardened specimen is a mixed one of transgranular and intergranular.
|
|
|
1 Gnanamuthu D S et al. In: Ferris S D et al, eds. Laser-Solid Interaction and Laser Processing, New York: AIP, 1979: 173 2 Kikuchi M et al. Proceedings of First Joint U.S./Japan International Laser Processing Conference, Toledo, Ohio, LIA, 1981 3 Cai Qing-kui, In: Barnby J T ed., Fatigue Prevention and Design, 1986: 333 4 #12 5 #12 6 董鄂,陈爱华.全国第三次高能密度热处理会议文集,长春,1991:60 7 Chilton J M, Kelly P M. Acta Metall 1986; 16: 637 8 Yokota M J, Lai G Y. Metall Trans, 1975; 6A: 1837 9 Lai G Y, Wood W E, Clark R A. Metall Trans 1974; 5: 1663 10 Bahre K. Z Werksto. fftech, 1978; 9: 45 11 刘常升.东北工学院博士论文,1992:41. |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|