| CORROSION FATIGUE CRACK PROPAGATION OF MARTENSITIC AND BAINITIC GC-4 ULTRA-HIGH STRENGTH STEEL |
| LIU Xiaokun;WANG Jianjun;LU Minxu;JIN Shi;FU Xiangjiong Xi'an Petroleum Institute Northwestern Polytechnical University; Xi'an |
|
Cite this article:
LIU Xiaokun;WANG Jianjun;LU Minxu;JIN Shi;FU Xiangjiong Xi'an Petroleum Institute Northwestern Polytechnical University; Xi'an. CORROSION FATIGUE CRACK PROPAGATION OF MARTENSITIC AND BAINITIC GC-4 ULTRA-HIGH STRENGTH STEEL. Acta Metall Sin, 1993, 29(12): 27-33.
|
|
|
Abstract The property and mechanism of corrosion fatigue (CF) crack propagation ofmartensitic and bainitic 40CrMnSiMoVA (GC-4) ultra-high strength steel was investigated.There is a platform region on CF crack propagation curve of the GC-4 steel with differentmicrostructure in 3.5% NaCl solution, which is similar to its stress corrosion crackingbehaviour. The CF crack propagation rate (in platform region) of martensitic GC-4 steel ismuch higher than that of bainitic one. Through fracture surface examination and theoreticalanalysis, it is revealed that hydrogen embrittlement plays an important role in the CF pro-cess of GC-4 steel.
|
|
|
1 Pawloski B, Mazur A, Gorczyca S. Corrosion Science, 1991, 32: 685 2 Bulloch J H. Theor Appl Fract Mech, 1991; 16: 1 3 Kerr R, Solana F. et al. Metall Trans, 1987; 18: 1011 4 郑文龙,朱国培,欧阳怀谨,李革.金属学报,1986;22:A275 5 陈大明.西北工业大学博士学位论文,1988 6 路民旭,刘晓坤,王建军等.航空学报,1990;11:12 7 王建军,刘晓坤,路民旭.航空学报,1988;9:13 8 Jin Shi, Liu Xiaokun. In: Goel V S ed., Proc Int Confon Fatigue, Corrosion Cracking, Fracture Failure Analysis, Salt Lake City, USA, 1985: 69 9 朱永昌.金属的应力腐蚀断裂.北京航空学院,1982 10 Solana F, et al. Metall Trans, 1987; 18A: 1023 11 Turnbull A. Br Corro J, 1980; 15: 162 12 Turnbull A. ASTM STP801, 1982 13 林栋梁,吴建生,杨正瑞.金属学报,1983;19:1 14 刘晓坤,王建军,金石.航空学报,1989;10:A479 15 刘晓坤.西北工业大学博士学位论文,1990? |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|