Abstract Superior hydrogen absorbability of the alloys of TiFe+xwt--%La with alternatelayer structure was found firstly. It would be available at 30℃ under 6 MPa H_2 without anyprior treatment.
|
|
Received: 18 April 1992
|
1 Bronca V, Bergman P, Ghaemmaghami V, Khatamian D, Manchester F D. J Less-Common Met, 1985; 108: 313--325 2 Raj P, Satyamoorthy A, Suryanarayana P, Singh A J, Iyer R M. J Less-Common Met, 1987; 130: 139--145 3 Hirata T. J Less-Common Met, 1987; 130: 497--502 4 Suzuki J, Abe M, Yamaguchi T, Terazawa S. J Less-Common Met, 1987; 131: 301--309 5 Nagai H, Kitagaki K, Shoji K. J Less-Common Met, 1987; 134: 275--296 6 钱久信,赵黎明,郑朝贵,叶于浦.金属学报,1984;20:A423 7 Sandrock G D. Final Report BNL 352410s (Brookhaven National Laboratory), Upton, New York, 197 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|