| EFFECT OF β-FLECK ON MECHANICAL PROPERTIES OF Ti-10V-2Fe-3Al ALLOY |
| ZHOU Yigang; YU Hanqing; ZENG Weidong (Northwestern Polytechnical University; Xi'an)TANG Jialing (Chinese Aviation South Power Machine Company; Zhuzhou) |
|
Cite this article:
ZHOU Yigang; YU Hanqing; ZENG Weidong (Northwestern Polytechnical University; Xi'an)TANG Jialing (Chinese Aviation South Power Machine Company; Zhuzhou). EFFECT OF β-FLECK ON MECHANICAL PROPERTIES OF Ti-10V-2Fe-3Al ALLOY. Acta Metall Sin, 1992, 28(12): 23-28.
|
|
|
Abstract Effect of β-fleck on properties of tensile elongation and low cycle fatigue life at room temperature for Ti-10V-2Fe-3Al alloy has been investigated. The cracks along initial β-grain boundaries in the β-fleck region may propagate to form intergranular brittle fracture. Under alternating load, the β-fleck often becomes a fatigue origin. While under higher strain, the cracks initiate and propagate to fracture early at the original β-grain boundaries in β-fleck region and at α-grain boundaries.
|
|
|
| 1 Froes F H, Bomberger H B. J Met, 1985; 37(7) :28
2 Bomberger H B, Froes F H. J Met, 1984; 36(12) :39
3 周义刚,俞汉清,张恒毕,徐好义.西北工业大学学报,1990;8(4) :425
4 Sparks R B, Long J R. Technical Reprit, AFML-TR-37-301, 1974
5 Funkenlusch A W, Coffio L F. Metall Trans, 1978; 9A:1159
6 Terlinde G T, Duerig T W, Williams J C. Metall Trans, 1983; 14A:2101
7 Craef M. Metall, 1978; 32:563
8 Feltner C E, Beardmor P. ASTM STP 467, 1969:77 |