Abstract  A three dimensional turbulent combustion mathematical model, which contained K-ε two equation model for turbulent flow, mixture fraction f, for combustion reaction and concentration fluctuation g, for turbulent combustion, was developed and successfully applied to post-combustion process in BOF, even though the model did not address problems, such as, radiation, multi-phase flow and finite reaction rate, as the ones exist in real process. Nevertheless, some interesting results of off-gases flow pattern, temperature profile, and the shape of the turbulent flame of post-combustion in BOF were worked out. Two controllable parameters, lance height and the angle of sub-hole to horizontal were studied.
Key words:  turbulent combustion      basic oxygen furnace      post-combustion      flame shape     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1992/V28/I12/29

1 Ito K, Fruehan R J. Metall Trans, 1989; 20B:509, 515
2 Szekely J. TMS Fall Extractive Meeting, Cologne, West Germany, Jom, 1990:16
3 Robertson T, Moore P, Hawkins R J. Ironmaking Steelmaking, 1986; 13:195
4 Takashiba N, Kojima S, Take H, Okuda H. In: Peter H Scholes ed., Steel Technology International 1989, Sterling Publication Int Ltd,
5 Turner G, Jahanshahi S. Trans Iron Steel lnst Jpn, 1987; 27:734
6 Hirai M, Tsujino R, Mukai T, Harada T, Omori M. Trans Iron Steel Inst Jpn, 1987; 27; 805
7 Koto Y, Grosjean J, Reboul J, Riboud P. Trans Iron Steel Inst Jpn, 1988; 28:287
8 Sugiyama S, Abe M, Nishioka S, Nakamura H, Takahashi K, Kawai Y. Trans Iron Steel lnst Jpn, 1987; 27:B-49
9 Spalding D B. Combust Sci Technol, 1976; 13:3
10 Pun W U, Spalding D B. In: Lunc M ed., Proc Int'l Astronautical Federation Meeting, Vol.Ⅲ, Belgrade, International Academy of Astronautical, Oxford: Pergamon, 1968:3-21
11 Gosman A D, Lockwood F C. In: Afgan N H ed., Proc Int'l Seminar on Heat Transfor From Flames, Torgir, Yugoslavia, New York: Wiley, 1974
12 Gosman A D, Lockwood F C. 14th Symposium (Int'l) on Combustion, Penn. State Univ., Combustion Institute, Pittsburgh, 1973:661-671
13 Spalding D B. Proc 13th Symposium (Int'l) on Combustion, The Univ. of Utah, Combustion Institute, Pittsburgh, 1971:649-657
14 Elghobashi S E, Pun W M. Proc 15th Symposium (Int'l) on Combustion, Tokyo, Combustion Institute, Pittsburgh, 1975:1353-1365
15 Khalil E E. Modeling of Furnaces and Combustors, Kent, Abacus Press, 1982
16 Gapta A K, Lilly D G. Flowfield Modeling and Diagnostics, Kent, Abacus Press, 1985
17 Spalding D B. Chem Eng Sci, 1971; 26:95
18 Reid R C, Prausnitz J M, Poling B E. The Properties of Gases and Liquids, New York, McGraw-Hill. 1986
[1] LI Baowei; HE Youduo(Baotou institute of Iron and Steel;Baotou 014010);Y. SAHAI(The Ohio State University; USA)(Manuscript received 1995-05-30). A MATHEMATICAL MODEL OF POST-COMBUSTION AT THE INITIAL STAGE IN TOP-BLOWN CONVERTER[J]. 金属学报, 1996, 32(2): 169-174.
No Suggested Reading articles found!