CRYSTALLIZATION OF METALLIC GLASS Zr_(70)Cu_(30) UNDER HIGH PRESSURE |
SHEN Dejiu; WU Haoquan (Yanshan University; Qinhuangdao); SHEN Zhongyi; CHEN Guiyu; YIN Xiujun (Institute of Physics; Academia Sinica; Beijing) |
|
Cite this article:
SHEN Dejiu; WU Haoquan (Yanshan University; Qinhuangdao); SHEN Zhongyi; CHEN Guiyu; YIN Xiujun (Institute of Physics; Academia Sinica; Beijing). CRYSTALLIZATION OF METALLIC GLASS Zr_(70)Cu_(30) UNDER HIGH PRESSURE. Acta Metall Sin, 1992, 28(10): 60-62.
|
Abstract Crystallization temperature of the metallic glass Zr_(70)Cu_(30), observed by X-ray diffraction analysis, may be increased about 20℃ under high pressure up to 2GPa. Besides α-Zr and CuZr_2 , the Cu_(10)Zr_7 phase was newly obtained as the another crystallization product.
|
Received: 18 October 1992
|
1 Cedergren M, Backstrom G. J Non-Cryst Solids, 1980; 37: 213 2 沈中毅,殷岫君,张云,洪景新,何寿安.物理学报,1985;34:1327 3 沈中毅,张云,殷岫君,何寿安,吴谦,吴自勤.物理学报,1983;32:1160 4 沈中毅,张云.科学通报,1981;26:913 5 沈德久,吴浩泉,郭景海,沈中毅.东北重型机械学院学报,1990;14:26 6 Freed R L, Vander J B. J Non-Cryst Solids, 1978; 27: 9 7 Altounian Z, Tu Guo-hua, Stron-Olsen J Q. J Appl Phys, 1982, 53: 4755 8 Wanson S. N B S Circular, 1953; 11: 539 9 Nevitt M V, Downey J W. Trans Met Soc AIME, 1962; 224: 195 10 Kirkpatrick M E. Smith J F, Larsen W L. Acta Cryst, 1962; 15: 894 11 Bsenko L. J Less-Comm Met, 1975; 40: 365V |