| STRUCTURAL ZONING DIAGRAM OF SOLID SOLUTION Fe-Mn-C ALLOY AT 1000℃ |
| LI Shaoxiong;HE Zhenming;ZHAO Yuguang;ZHAO Yuqian;SHI Zhongliang Jilin University of Technology; Changchun |
|
Cite this article:
LI Shaoxiong;HE Zhenming;ZHAO Yuguang;ZHAO Yuqian;SHI Zhongliang Jilin University of Technology; Changchun. STRUCTURAL ZONING DIAGRAM OF SOLID SOLUTION Fe-Mn-C ALLOY AT 1000℃. Acta Metall Sin, 1991, 27(5): 90-94.
|
|
|
Abstract On the basis of experimental results of 76 points of composition and previous relevant conclusions, a complete structural zoning diagram of solid solution treating Fe-Mn-C system alloy at 1000℃ has been constructed with austenite zones of different stabilities. The chemical composition range and structure change of various Mn steels have also been discussed. Thus, the reasonable selection of composition and structure may be available for the Mn steel with commercial purposes.
|
|
Received: 18 May 1991
|
1 张鸿冰,倪乐民,徐祖耀.金属学报,1987;23:A42-49 2 陈希杰.高锰钢.北京:机械工业出版社,1989:5-7,68-71,351-359 3 #12 4 #12 5 李隆盛.铸造合金及熔炼.北京:机械工业出版社,1989:170 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|