COMPLEX FORMED IN EXTRACTION OF DIVALENT Mn BY ALKYLPHOSPHONIC ACID MONOESTER
HUANG Kelong;SHU Wanyin;DING Dunhuang;LIU Guogen;DONG Ping Central South University of Technology; Changsha
Cite this article: 

HUANG Kelong;SHU Wanyin;DING Dunhuang;LIU Guogen;DONG Ping Central South University of Technology; Changsha. COMPLEX FORMED IN EXTRACTION OF DIVALENT Mn BY ALKYLPHOSPHONIC ACID MONOESTER. Acta Metall Sin, 1991, 27(4): 88-92.

Download:  PDF(441KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  In order to clarify the mechanism and the complex formed in the ex-traction of divalent Mn by alkylphosphonic acid monoester, the solid complex hasbeen prepared by mono (2-ethylhexyl)-2-ethylhexyl phosphate, HEH(EH)P, HA withdivalent Mn. The elemental analysis, magnetic susceptibility and thermogravimetryhave been determined for the solid complex of HEH(EH)P-Mn(Ⅱ) and the infraredspectrum has been carried out in comparison to the extractant HEH(EH)P. The extra-cted compound has also been studied by electronic and electron spin resonance spec-troscopy in octane solvent and solid state at room temperature. On the basis of themeasurements, it is concluded that the structure of the solid polymeric species MnA_2is in a tetrahedral arrangement.
Key words:  solvent extraction      mono(2-ethylhexyl)-2-ethylhexyl phosphate      Mn      extracted complex     
Received:  18 April 1991     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1991/V27/I4/88

1 黄可龙,舒万银,张祥麟.化学学报,1989;47(1) :67
2 Sato T, Ueda M. In: Thornton J D, Naylor A, Mckay H A C, Jeffreys G V eds., Proceedings of the International Solvent Extraction Conference, ISEC74, Vol. Ⅰ, London: Society of Chemistry Industry. 1974: 871
3 马恩新,严小敏,王三益,龙海燕,袁承业.中国科学,1981;(5) :565
4 Kolarik Z, Crimm R.J Inorg Nucl Chem, 1976; 38: 1721
5 张祥麟,康衡主编.配位化学.长沙:中南工业大学出版社,1986:603
6 Furlani C, Furlani A. J Inorg Nucl Chem, 1961; 19: 51
7 Chan S I, Fung B M, Lutje H. J Chem Phys, 1967; 47: 2121r
[1] DING Hua, ZHANG Yu, CAI Minghui, TANG Zhengyou. Research Progress and Prospects of Austenite-Based Fe-Mn-Al-C Lightweight Steels[J]. 金属学报, 2023, 59(8): 1027-1041.
[2] LI Xiaohan, CAO Gongwang, GUO Mingxiao, PENG Yunchao, MA Kaijun, WANG Zhenyao. Initial Corrosion Behavior of Carbon Steel Q235, Pipeline Steel L415, and Pressure Vessel Steel 16MnNi Under High Humidity and High Irradiation Coastal-Industrial Atmosphere in Zhanjiang[J]. 金属学报, 2023, 59(7): 884-892.
[3] CHENG Yuanyao, ZHAO Gang, XU Deming, MAO Xinping, LI Guangqiang. Effect of Austenitizing Temperature on Microstructures and Mechanical Properties of Si-Mn Hot-Rolled Plate After Quenching and Partitioning Treatment[J]. 金属学报, 2023, 59(3): 413-423.
[4] CHEN Xueshuang, HUANG Xingmin, LIU Junjie, LV Chao, ZHANG Juan. Microstructure Regulation and Strengthening Mechanisms of a Hot-Rolled & Intercritical Annealed Medium-Mn Steel Containing Mn-Segregation Band[J]. 金属学报, 2023, 59(11): 1448-1456.
[5] HAN Dong, ZHANG Yanjie, LI Xiaowu. Effect of Short-Range Ordering on the Tension-Tension Fatigue Deformation Behavior and Damage Mechanisms of Cu-Mn Alloys with High Stacking Fault Energies[J]. 金属学报, 2022, 58(9): 1208-1220.
[6] GENG Yaoxiang, TANG Hao, XU Junhua, ZHANG Zhijie, YU Lihua, JU Hongbo, JIANG Le, JIAN Jianglin. Formability and Mechanical Properties of High-Strength Al-(Mn, Mg)-(Sc, Zr) Alloy Produced by Selective Laser Melting[J]. 金属学报, 2022, 58(8): 1044-1054.
[7] REN Ping, CHEN Xingpin, WANG Cunyu, YU Feng, CAO Wenquan. Effects of Pre-Strain and Two-Step Aging on Microstructure and Mechanical Properties of Fe-30Mn-11Al-1.2C Austenitic Low-Density Steel[J]. 金属学报, 2022, 58(6): 771-780.
[8] GUO Dongwei, GUO Kunhui, ZHANG Fuli, ZHANG Fei, CAO Jianghai, HOU Zibing. A New Method for CET Position Determination of Continuous Casting Billet Based on the Variation Characteristics of Secondary Dendrite Arm Spacing[J]. 金属学报, 2022, 58(6): 827-836.
[9] SUN Yi, ZHENG Qinyuan, HU Baojia, WANG Ping, ZHENG Chengwu, LI Dianzhong. Mechanism of Dynamic Strain-Induced Ferrite Transformation in a 3Mn-0.2C Medium Mn Steel[J]. 金属学报, 2022, 58(5): 649-659.
[10] SHEN Guohui, HU Bin, YANG Zhanbing, LUO Haiwen. Influence of Tempering Temperature on Mechanical Properties and Microstructures of High-Al-Contained Medium Mn Steel Having δ-Ferrite[J]. 金属学报, 2022, 58(2): 165-174.
[11] JIANG Weining, WU Xiaolong, YANG Ping, GU Xinfu, XIE Qingge. Formation of Dynamic Recrystallization Zone and Characteristics of Shear Texture in Surface Layer of Hot-Rolled Silicon Steel[J]. 金属学报, 2022, 58(12): 1545-1556.
[12] WANG Yu, HU Bin, LIU Xingyi, ZHANG Hao, ZHANG Haoyun, GUAN Zhiqiang, LUO Haiwen. Influence of Annealing Temperature on Both Mechanical and Damping Properties of Nb-Alloyed High Mn Steel[J]. 金属学报, 2021, 57(12): 1588-1594.
[13] WANG Shihong, LI Jian, CHAI Feng, LUO Xiaobing, YANG Caifu, SU Hang. Influence of Solution Temperature on γ→ε Transformation and Damping Capacity of Fe-19Mn Alloy[J]. 金属学报, 2020, 56(9): 1217-1226.
[14] DENG Yahui, YANG Yinhui, PU Chaobo, NI Ke, PAN Xiaoyu. Effect of Mn Addition on High Temperature Tensile Behavior of 23%Cr Low Nickel Type Duplex Stainless Steel[J]. 金属学报, 2020, 56(7): 949-959.
[15] YAO Xiaofei, WEI Jingpeng, LV Yukun, LI Tianye. Precipitation σ Phase Evoluation and Mechanical Properties of (CoCrFeMnNi)97.02Mo2.98 High Entropy Alloy[J]. 金属学报, 2020, 56(5): 769-775.
No Suggested Reading articles found!