| KINETICS OF DESULPHURIZING REACTION OF BLAST FURNACE LOW TITANIA SLAG |
| YAN Yuzhang;LAN Hong Chongqing University |
|
Cite this article:
YAN Yuzhang;LAN Hong Chongqing University. KINETICS OF DESULPHURIZING REACTION OF BLAST FURNACE LOW TITANIA SLAG. Acta Metall Sin, 1991, 27(4): 80-83.
|
|
|
Abstract A The desulphurizing reaction of the blast furnce low titania slag underthe condition of no external agitation is confirmed to be of a first order. The con-trolling step is the diffusion of S in slag. The measures to accelerate the rate ofdesulphurization are approached.
|
|
Received: 18 April 1991
|
1 Ramachandran S, King T B, Grant N J. Trans AIME. 1956: 206: 1548 2 羽田野道春.铁钢,1969;55(11) :314 3 Chang L, Goldman K M. Trans AIME, 1984; 176: 309 4 川合保治.铁钢,1984;70:1640 5 林衍先,尹文超.钢铁,1987;(2) :1 |