Abstract The morphology and substructure of martensites in 7CrSiMnMoV steelwere observed under optical or electron microscope, and martensitic transformationwith its morphology was also analysed. In the normally quenched steel three typesof martensites are found, including the wide lath one of dislocation substructure form-ed preferentially along grain boundaries, the thinner inner laths and the twinningmartensite plate in interior of grain. Therefore, an attempt was made to substitutelower bainite, formed by short-term isothermal quenching, for intergranular marten-site, it is believed that the morphology would be very influential to the strength-toughness of the steel.
|
|
Received: 18 March 1991
|
1 章守华.金属热处理.北京:中国工业出版社,1965:50-54 2 王桂金.材料科学与工程,1986;(4) :1-12 3 Gu Nanju. Proc ICOMAT-86, Nara, Japan, 1986, The Japan Inst Metals, 1987: 325 4 贡海,谷南驹.金属学报,1987;23:A374 5 谷南驹,王瑞祥,殷福星.金属学报,1991;27(3) :A 6 Zhang X M, Gautier E, Simon A. Acta Metall, 1989; 37: 477--485 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|