EFFECT OF HETEROGENEOUS DISTRIBUTION OF C AND ALLOYING ELEMENTS ON γ/α′ TRANSFORMATION IN A Fe-Mn-Cr-C ALLOY
ZHENG Yasgzeng;ZHANG Fucheng Yanshan University; Qinhuangdao
Cite this article: 

ZHENG Yasgzeng;ZHANG Fucheng Yanshan University; Qinhuangdao. EFFECT OF HETEROGENEOUS DISTRIBUTION OF C AND ALLOYING ELEMENTS ON γ/α′ TRANSFORMATION IN A Fe-Mn-Cr-C ALLOY. Acta Metall Sin, 1991, 27(3): 82-85.

Download:  PDF(328KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The heterogeneous distribution of C and metallic alloying elements as well asthe phase composition changed before and after cold deformation of a Fe-Mn-Cr-C alloyhave been studied by Mossbauer spectroscopy. The austenites without and with C and metallicalloying elements are found in the alloy as solid solution treated state. While the martensiteswithout and with C and alloying elements may be induced by cold deformation. The transforma-tion from austenite to martensite in the alloy is confirmed via theoretical computation andexperiments to be controlled by the number of covalent electron pairs forming covalent bondin austenitic crystal cell of the alloy. The formation of strong covalent bond between C andmetallic elements will vigorously retard the γ/α′transformation.
Key words:  heterogeneity      solid solution      Mossbauer spectroscopy      strain induced martensite      valence electron structure     
Received:  18 March 1991     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1991/V27/I3/82

1 刘志林,牛洪军,金灿风,王斌.科学通报,1987;32:1787
2 张福成,郑炀曾.科学通报,1991;23:382
3 刘志林,戴天时,牛洪军,金灿风.机械工程学报,1989;25(1) :29
4 Ino H, Moriya T, Fujita E F, Maeda Y, Ono Y. Inokuti Y. J Phys Soc Jpn. 1968; 25: 88
5 余瑞璜.科学通报,1978;23:217
6 Vincze J, Campbell I A. J Phys F: Metal Phys, 1973; 3: 647I
[1] HAN Linzhi, MU Juan, ZHOU Yongkang, ZHU Zhengwang, ZHANG Haifeng. Effect of Heat Treatment Temperature on Microstructure and Mechanical Properties of Ti0.5Zr1.5NbTa0.5Sn0.2 High-Entropy Alloy[J]. 金属学报, 2022, 58(9): 1159-1168.
[2] ZHANG Haijun, QIU Shi, SUN Zhimei, HU Qingmiao, YANG Rui. First-Principles Study on Free Energy and Elastic Properties of Disordered β-Ti1-xNbx Alloy: Comparison Between SQS and CPA[J]. 金属学报, 2020, 56(9): 1304-1312.
[3] CAO Tieshan, ZHAO Jinyi, CHENG Congqian, MENG Xianming, ZHAO Jie. Effect of Cold Deformation and Solid Solution Temperature on σ-phase Precipitation Behavior in HR3C Heat Resistant Steel[J]. 金属学报, 2020, 56(5): 673-682.
[4] Miao JIN, Wenquan LI, Shuo HAO, Ruixue MEI, Na LI, Lei CHEN. Effect of Solution Temperature on Tensile Deformation Behavior of Mn-N Bearing Duplex Stainless Steel[J]. 金属学报, 2019, 55(4): 436-444.
[5] Min ZHANG, Erlong MU, Xiaowei WANG, Ting HAN, Hailong LUO. Microstructure and Mechanical Property of the Welding Joint of TA1/Cu/ X65 Trimetallic Sheets[J]. 金属学报, 2018, 54(7): 1068-1076.
[6] Chuang DONG, Dandan DONG, Qing WANG. Chemical Units in Solid Solutions andAlloy Composition Design[J]. 金属学报, 2018, 54(2): 293-300.
[7] Yinhui ZHANG, Qiang FENG. Effects of W on Creep Behaviors of Novel Nb-Bearing Austenitic Heat-Resistant Cast Steels at 1000 ℃[J]. 金属学报, 2017, 53(9): 1025-1037.
[8] Hongwei ZHANG,Xuezhi QIN,Xiaowu LI,Lanzhang ZHOU. Incipient Melting Behavior and Its Influences on the Mechanical Properties of a Directionally Solidified Ni-Based Superalloy with High Boron Content[J]. 金属学报, 2017, 53(6): 684-694.
[9] Zongyue BI,Jun YANG,Haizhang LIU,Wanpeng ZHANG,Yaobin YANG,Lei TIAN,Xiaojiang HUANG. INVESTIGATION ON THE WELDING PROCESS AND MICROSTRUCTURE AND MECHANICAL PROPERTY OF BUTT JOINTS OF TA1/X65 CLAD PLATES[J]. 金属学报, 2016, 52(8): 1017-1024.
[10] Xiaohong YOU,Ganggang WANG,Jun WANG,Tao XU,Hongyu ZHANG,Hua WEI. EFFECT OF SOLID SOLUTION TREATMENT ONMICROSTRUCTURE AND MECHANICALPROPERTIES OF HOT-PRESS CoCrW ALLOYS[J]. 金属学报, 2016, 52(2): 161-167.
[11] Shoudong CHEN,Xianghua LIU,Lizhong LIU,Meng SONG. CRYSTAL PLASTICITY FINITE ELEMENT SIMULA- TION OF SLIP AND DEFORMATION IN ULTRA- THIN COPPER STRIP ROLLING[J]. 金属学报, 2016, 52(1): 120-128.
[12] LI Weijuan, ZHANG Hengyi, FU Hao, ZHANG Jianping, QI Xiangyu. INTERNAL FRICTION STUDY OF MECHANISM OF BAKE-HARDENING ON LOW CARBON STEEL[J]. 金属学报, 2015, 51(4): 385-392.
[13] Xiaogang WANG,Chao JIANG,Xu HAN. PLASTIC STRAIN HETEROGENEITY AND WORK HARDENING OF Ni SINGLE CRYSTALS[J]. 金属学报, 2015, 51(12): 1457-1464.
[14] YANG Fuqiang, SONG Renbo, SUN Ting, ZHANG Leifeng, ZHAO Chao, LIAO Baoxin. MICROSTRUCTURE AND MECHANICAL PROPER- TIES OF Fe-Mn-Al LIGHT-WEIGHT HIGH STRENGTH STEEL[J]. 金属学报, 2014, 50(8): 897-904.
[15] JIE Jinchuan, ZOU Chunming, WANG Hongwei, WEI Zunjie. MECHANICAL BEHAVIOR OF Al-20Mg ALLOY SOLIDIFIED UNDER HIGH PRESSURE[J]. 金属学报, 2014, 50(8): 971-978.
No Suggested Reading articles found!