SUBSTRUCTURAL AND CRYSTALLOGRAPHIC FEATURES OF LOWER BAINITE
SUN Jialin Kunming Institute of Technology; KANG Mokuang Northwestern Polytechnical University; Xi'an
Cite this article: 

SUN Jialin Kunming Institute of Technology; KANG Mokuang Northwestern Polytechnical University; Xi'an. SUBSTRUCTURAL AND CRYSTALLOGRAPHIC FEATURES OF LOWER BAINITE. Acta Metall Sin, 1991, 27(3): 72-76.

Download:  PDF(773KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Based on the TEM analysis of substructures of lower bainite in twosteels containing Si, the lattice invariant shear elements were determined and a plasticaccommodation double-shear model was proposed. The theorotical predictions aboutcrystallography given by the model are in good agreement with the experimental da-ta for the steels tested.
Key words:  bainite transformation      substructure      crystallography     
Received:  18 March 1991     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1991/V27/I3/72

1 Bowles J S, Kennon N F. J Aust Inst Met, 1960; 5: 106
2 Srinivasan G R, Wayman C M. Acta Metall, 1968; 16: 609, 621
3 Ross N D H, Crocker A G. Acta Metall, 1970; 18: 405
4 Ohmori Y. Trans Iron Steel Inst Jpn, 1971; 11: 95
5 Hoekstra S. Acta Metall, 1980; 28: 507
6 孙加林.西北工业大学博士学位论文,1989
7 Sandvik B P J. Metall Trans, 1982; 13A: 777
8 Sandvik B P J, Wayman C M. Metall Trans, 1983; 14A: 809
9 Wechsler M S, Lieberman D S, Read T A. Trans AIME, 1953; 197: 1503
10 Bowles J S, Mackenzie J K. Acta Metall, 1954; 2: 129, 138, 224
11 Sandvik B P J, Wayman C M. Metall Trans, 1983; 14A: 2469
12 康沫狂,杨思品,管敦惠.纲中贝氏体,上海,上海科学技术出版社,1990
[1] LI Xueda, LI Chunyu, CAO Ning, LIN Xueqiang, SUN Jianbo. Crystallography of Reverted Austenite in the Intercritically Reheated Coarse-Grained Heat-Affected Zone of High Strength Pipeline Steel[J]. 金属学报, 2021, 57(8): 967-976.
[2] Wensheng XU, Wenzheng ZHANG. An Investigation of the Crystallography of Pearlites Nucleated on the Proeutectoid Cementite[J]. 金属学报, 2019, 55(4): 496-510.
[3] Huidong WU, Goro MIYAMOTO, Zhigang YANG, Chi ZHANG, Hao CHEN, Tadashi FURUHARA. Incomplete Bainite Transformation Accompanied with Cementite Precipitation in Fe-1.5(3.0)%Si-0.4%C Alloys[J]. 金属学报, 2018, 54(3): 367-376.
[4] Zhaozhao WEI, Xiao MA, Xinping ZHANG. Topological Modelling of the B2-B19' Martensite Transformation Crystallography in NiTi Alloy[J]. 金属学报, 2018, 54(10): 1461-1470.
[5] WEI Zhaozhao, MA Xiao, ZHANG Xinping. STUDY ON THE DISLOCATION STRUCTURE OF INTERPHASE INTERFACE AND MARTENSITE TRANSFORMATION CRYSTALLOGRAPHY IN Ni2 MnGa ALLOY[J]. 金属学报, 2013, 49(2): 187-198.
[6] LU Fayun, YANG Ping, MENG Li, WANG Huizhen. MICROSTRUCTURE, MECHANICAL PROPERTIES AND CRYSTALLOGRAPHY ANALYSIS OF Fe-22Mn TRIP/TWIP STEEL AFTER TENSILE DEFORMATION[J]. 金属学报, 2013, 49(1): 1-9.
[7] GU Xinfu ZHANG Wenzheng. A SIMPLE VECTOR ANALYSIS METHOD FOR MARTENSITE CRYSTALLOGRAPHY[J]. 金属学报, 2011, 47(2): 241-245.
[8] SHI Zhangzhi ZHANG Wenzheng. DESIGNING Mg-Sn-Mn ALLOY BASED ON CRYSTALLOGRAPHY OF PHASE TRANSFORMATION[J]. 金属学报, 2011, 47(1): 41-46.
[9] WANG Liuding DING Fucai WANG Baimin ZHU Ming ZHONG Yingliang LIANG Jinkui. INFLUENCE OF SUPER--FINE SUBSTRUCTURE ON TOUGHNESS OF LOW--ALLOYING ULTRA--HIGH STRENGTH STRUCTURE STEEL[J]. 金属学报, 2009, 45(3): 292-296.
[10] KANG Mokuang ZHANG Mingxing LIU Feng ZHU Ming. OVERALL ACTIVATION ENERGY OF ISOTHERMAL TRANSFORMATION IN METAL ALLOY AND ITS MECHANISM I. Medium Temperature (Bainite) Isothermal Transformation in Steels[J]. 金属学报, 2009, 45(1): 25-31.
[11] Dong Qiu; Wenzheng Zhang. Research Progress in Precipitation Crystallography models[J]. 金属学报, 2006, 42(4): 341-349 .
[12] YANG Jinbo; YANG Zhigang; QIU Dong; ZHANG Wenzheng; ZHANG Chi; BAI Bingzhe; FANG Hongsheng. A general crystallographic model of fcc/bcc(bct) martensitic nucleation and growth in steels[J]. 金属学报, 2005, 41(3): 225-230 .
[13] LUO Chengping(C.P.Luo);LIU Jiangwen;XIAO Xiaoling(Department of Mechanical Engineering; South China University of Technology; Guangzhou 510641)Correspondent:LUO Chengping; professor; Tel:(020)85511617; Fax: (020)87111312;E-mail: mecpluo@letterbox.scut.edu.cn. FINE STRUCTURE AND CRYSTALLOGRAPHY OF ISOTHERMAL LOWER BAINITE IN AN EXPERIMENTAL STEEL 38Si2Mn2Mo[J]. 金属学报, 1998, 34(10): 1009-1015.
[14] ZUO Rulin; ZHOU Shouze; DING Peidao (Department of Metallurgy and Materials Engineering; Chongqing University; Chongqing 630044). SHEAR PROCESS OF FERROUS MARTENSITES[J]. 金属学报, 1996, 32(9): 904-912.
[15] XU Yongbo;BAI Yilong;SHEN Letian;XUE Qing;LI Huan;KONG Dan( State Key Laboratory for Fatigue and Fracture of Materials;Institute of Metal Research;Chinese Academy of Sciences; Shenyang 110015)(Laboratory for Non-Linear Mechanics of Continuous Media;Institute of Mechanics;Chinese Academy of Sciences;Beijing 100080)(Manuscript received 1994-10-28;in revised form 1995-04-01). FORMATION AND DEVELOPMENT OF SHEAR DEFORMATION LOCALIZATION IN LOW CARBON STEELS[J]. 金属学报, 1995, 31(11): 485-493.
No Suggested Reading articles found!