| CORROSION BEHAVIOUR OF M38 SUPERALLOY IN SO_2+O_2 MIXED ENVIRONMENT AT ELEVATED TEMPERATURES |
| QI Huibin;LI Tiefan Institute of Corrosion and Protection of Metals; Laboratory for Corrosion Science; Academia Sinica; Shenyang |
|
Cite this article:
QI Huibin;LI Tiefan Institute of Corrosion and Protection of Metals; Laboratory for Corrosion Science; Academia Sinica; Shenyang. CORROSION BEHAVIOUR OF M38 SUPERALLOY IN SO_2+O_2 MIXED ENVIRONMENT AT ELEVATED TEMPERATURES. Acta Metall Sin, 1991, 27(2): 114-118.
|
|
|
Abstract The high temperature corrosion behaviour of the Ni-base casting su-peralloy M38 has been studied under the equilibrium SO_2+O_2 mixed gaseous environ-ment in the temperature range of 700-900℃. The kinetic curve, measured by non-continuous weighing, obeys the parabolic law. A corrosion mechanism was pro-posed and the effects of Al, Ti and Ta were also discussed.
|
|
Received: 18 February 1991
|
1 冶金工业部钢铁研究总院等编.高温合金金相图谱.北京:冶金工业出版社,1979 2 Natesan K. In: Rapp R A ed, High Temperature Corrosion, Houston, Texas: National Association Corrosion Engineers, 1983: 336 3 Luthra K L, Worrell W L. Metall Trans, 1979; 10A; 621 4 Luthra K L, Worrell W L. Metall Trans, 1978; 9A: 1055 5 Sidky P S, Hocking M G. Corros Sci, 1987; 27: 187 6 Hocking M G, S?dky P S. Corros Sci, 1987; 27: 205 7 Alcock C B, Hocking M G, Zador S. Corros Sci, 1969; 9: 111 8 Hocking M G, Vasantasree V. Corros Sci. 1976; 16: 279 9 Giggins C S, Pettit F S. Oxid Met. 1980; 14: 363 10 方炜.中国科学院金属研究所硕士论文,1987? |
| No Suggested Reading articles found! |
|
|